Re: Nondestructive testing of railroad wheels at the German Bahn AG
Posted by: Christian Grosse , E-mail: christian.grosse@po.uni-stuttgart.de, on June 08, 1998 at 11:06:46:In Reply to: Re: Nondestructive testing of railroad wheels at the German Bahn AG posted by : Rolf Diederichs on June 08, 1998 at 08:19:54:
>
>Based on the information available to us, we know that in Hamburg and Munich UT systems have worked since 1992.
>Anyone have some details about the UT systems the Deutsche Bahn AG is
using for inspection? What type of measuring device and transducers are
used?Regards
Chr. Grosse
--------------
Dr. Christian Grosse
Institut fuer Werkstoffe im Bauwesen (Construction Materials)
Universitaet Stuttgart (University of Stuttgart)
+++ phone/fax/address at:
http://www.uni-stuttgart.de/UNIuser/fmpa/grosse/grosse.html
- Update Rolf Diederichs 12:44:31 6/08/98
(7)