Query: Vibration testing of wood
Posted by: Ong Chee Beng(PID_1099), E-mail: ongcb@frim.gov.my, on December 22, 2001 at 04:44 :
Hello,
I am trying to calculate the Young's Modulus of wood using the NDT method of bending vibrations from the frequency of vibration. Anyone can provide me to any related literature available.
I only have the diferrential equation of bending vibrations by Goens, E., 1931: Determination of Young's Modulus from Flexural Vibrations. Ann. Phys. 11: 649 - 78) but didn't have the whole aritcle. Can anyone send me the paper?
Thanks in advance.
ong