ultrasonic testing of butt weld in cross country pipeline

Posted by: rajeev chaudhari Profile (PID_793), E-mail: otislab@vsnl.net, on December 23, 2001 at 11:58 :

dear friends,
please let me know the instruments, techniques for testing butt weld joints in cross country pipeline. I will appreciate to recieve details at my address as below.

R.J.Chaudhari
Offshore Testing & Inspection Services (I) Pvt. Ltd.,
W-147, MIDC Pawane,
Thane Belapur Road,
Navi Mumbai 400 703
India
Tel: +91 22 7670874 / 7681946
Fax: +91 22 7633982



Follow Ups:



Post a Followup:

Name:
E-Mail:

Subject:

Comments:

Optional Link URL: Example: "http://www....html". Alternative write "http://www.ndt.net/wshop/attach/filename.htm" if you transfered a filename.htm via FTP
Link Title: is important! Information on my Home Page
Optional Image URL: http://www....gif


Attention! Please click the button only once. This may take a moment to process


[ NDT-net Forum ] [ Help ]