[ NDT-net Forum ]
[ Follow Ups ] [ Post Followup ] [ Help ]
Re: ultrasonic testing of butt weld in cross country pipeline
Posted by: Ed T. , E-mail: trotteje@yahoo.com, on December 24, 2001 at 11:02 :In Reply to: Re: ultrasonic testing of butt weld in cross country pipeline posted by : Ed Trotter , E-mail: trotteje@yahoo.com, on December 24, 2001 at 04:21 :
: : dear friends,
: : please let me know the instruments, techniques for testing butt weld joints in cross country pipeline. I will appreciate to recieve details at my address as below.
: .
: : R.J.Chaudhari
: : Offshore Testing & Inspection Services (I) Pvt. Ltd.,
: : W-147, MIDC Pawane,
: : Thane Belapur Road,
: : Navi Mumbai 400 703
: : India
: : Tel: +91 22 7670874 / 7681946
: : Fax: +91 22 7633982
: .
: Are you talking about manual stick welding or mechanized GMAWs welding?
. You can use whatever RT setup you want for the manual welding depending on the speed of your spreads. Maybe a crawler, but for the GMAW-s you ought to be looking into automated UT. Some of the IF encountered with this process, especially with the heavier wall pipe is difficult and sometimes impossible to detect with RT.
Bright Technical Services