[ NDT-net Forum ]
[ Follow Ups ] [ Post Followup ] [ Help ]

Re: ultrasonic testing of butt weld in cross country pipeline

Posted by: Oleg Volf Profile (PID_1094), E-mail: ovolf@hotmail.com, on December 28, 2001 at 17:19 :

In Reply to: ultrasonic testing of butt weld in cross country pipeline posted by : rajeev chaudhari Profile , E-mail: otislab@vsnl.net, on December 23, 2001 at 11:58 :

Please check www.shawpipeline.com
We provide RT and AUT service for weld inspection.