Re: Thickness IQI Based on
Posted by: Zeki Cosku Gokce , E-mail: photographer21@yahoo.com, on November 29, 2003 at 05:48 :In Reply to: Thickness IQI Based on posted by : Mehmet Bal
, E-mail: malibal@tr.net, on November 28, 2003 at 22:29 :
Mehmet Bey,
According to ASME-V article-2 T-276 (a) The thickness on which the IQI is based on the nominal single wall thickness plus the estimated weld reinforcement….. Actual weld measurement of the weld reinforcement is not required.
So in your case (10.31 mm) you can use set B type of panateremeter.Regrads,
Zeki Cosku Gokce
----------- Start Original Message -----------
: Can any one answer the following: 2 inches but weld is radiograped eliptically. The wall thickness is 8.71 mm and weld reinsforcemnt is 1.6mm. In accordance with ASME-V article-2 T-276 what will be the thickness that the penetrameter based on. In another way the thickness that the penetrameter based on will be (8.71mm+1.6mm=10.31mm) or (8.71mm+8.71mm+1.6mm=19.02mm)?
: Looking forward to have your answer with appreciation.
: Many Thanks in advance
: Mehmet Bal
------------ End Original Message ------------
- Re: Thickness IQI Based on Ed T. 00:26 Dec-07-2003 (19)
- Re: Thickness IQI Based on Diana King 08:19 Aug-01-2004 (0)
- Re: Thickness IQI Based on Zeki Cosku Gokce 08:02 Dec-10-2003 (17)
- Re: Thickness IQI Based on Mehmet Bal
20:19 Dec-11-2003 (7)
- Re: Thickness IQI Based on Nancy MacCrimmon 08:08 Aug-01-2004 (0)
- Re: Thickness IQI Based on S.V.Swamy
15:35 Dec-15-2003 (5)
- Re: Thickness IQI Based on Mehmet Bal
21:48 Dec-15-2003 (4)
- Re: Thickness IQI Based on S.V.Swamy
15:34 Dec-16-2003 (3)
- Re: Thickness IQI Based on steve hornby
23:00 Dec-16-2003 (2)
- Re: Thickness IQI Based on Ed T. 00:12 Dec-19-2003 (1)
- Re: Thickness IQI Based on Ed T. 00:14 Dec-19-2003 (0)
- Re: Thickness IQI Based on Sasaki 01:50 Dec-11-2003 (8)
- Re: Thickness IQI Based on Ed T. 08:37 Dec-19-2003 (7)
- Re: Thickness IQI Based on N. Kuppusamy
03:01 Dec-22-2003 (6)
- Re: Thickness IQI Based on S.V.Swamy
15:12 Dec-23-2003 (5)
- Re: Thickness IQI Based on Jessica South 02:36 Aug-10-2004 (0)
- Re: Thickness IQI Based on Sasaki 05:00 Dec-26-2003 (3)
- Re: Thickness IQI Based on Ciara Bunnell 01:19 Aug-10-2004 (0)
- Re: Thickness IQI Based on Mehmet Bal
14:14 Dec-26-2003 (1)
- Re: Thickness IQI Based on Sasaki 01:13 Dec-27-2003 (0)
Attention! Please click the button only once. This may take a moment to process
[ Technical Discussions ] [ All Message Boards ] [ Help ]