[ Technical Discussions ]
[ Follow Ups ] [ Post Followup ] [ Help ]
Re: Thickness IQI Based on
Posted by: Sasaki , E-mail: sasaki.0125@plantech.co.jp, on December 11, 2003 at 01:50 :In Reply to: Re: Thickness IQI Based on posted by : Zeki Cosku Gokce , E-mail: photographer21@yahoo.com, on December 10, 2003 at 08:02 :
The "interpretation" of ASME Section V clearly defines the "Material thickness" in question.
The height of weld reinforcement at both sides of plate is applicable to X-groove weld ONLY.
Therefore, 10.31mm is a correct "material thickness", pipe wall thickness plus outside weld reinforcement height, for IQI selection.
- Re: Thickness IQI Based on Ed T. 08:37 Dec-19-2003 (7)
- Re: Thickness IQI Based on N. Kuppusamy
03:01 Dec-22-2003 (6)
- Re: Thickness IQI Based on S.V.Swamy
15:12 Dec-23-2003 (5)
- Re: Thickness IQI Based on Jessica South 02:36 Aug-10-2004 (0)
- Re: Thickness IQI Based on Sasaki 05:00 Dec-26-2003 (3)
- Re: Thickness IQI Based on Ciara Bunnell 01:19 Aug-10-2004 (0)
- Re: Thickness IQI Based on Mehmet Bal
14:14 Dec-26-2003 (1)
- Re: Thickness IQI Based on Sasaki 01:13 Dec-27-2003 (0)