Forum
General Discussions
Re: EMAT
Posted by: Larry Hopper , E-mail: Address, on November 07, 2008 at 14:32 :In Reply to: EMAT posted by : Filipe Matta
, E-mail: Address, on November 05, 2008 at 16:12 :
----------- Start Original Message -----------
: I'm looking for EMAT devices to inspect pressure vessels for flaw detections on welds and thickness reduction on walls of these equipments. This is to avoid using other tests like hidraulic and radiographic tests.
: Can someone give me information on companies who provide EMAT devices that fulfill my needs?
: Thanks
: Filipe
------------ End Original Message ------------There is another alternative that is very effective. The alternative is Low Frequency Electromagnetics. This is used all over the world for tank wall scanning. Secondly, Balanced field eddy current is available for weld crack inspections. Contact TesTex for more information.
- Re: EMAT Joe Buckley
![]()
16:32 Nov-07-2008 (0)
Attention! Please click the button only once. This may take a moment to process