Posted by: Mark Potter , E-mail: Address, on November 09, 2008 at 13:11 :

In Reply to: EMAT posted by : Filipe Matta Profile , E-mail: Address, on November 05, 2008 at 16:12 :

Dear Filipe,

we make EMAT based inspection systems - if the pressure vessels are steel, we have an off-the-shelf system that should be suitable for wall thinning, and can make weld inspection EMAT systems bespoke.

Sincerely,

Mark

----------- Start Original Message -----------
: I'm looking for EMAT devices to inspect pressure vessels for flaw detections on welds and thickness reduction on walls of these equipments. This is to avoid using other tests like hidraulic and radiographic tests.
: Can someone give me information on companies who provide EMAT devices that fulfill my needs?
: Thanks
: Filipe
------------ End Original Message ------------




Follow Ups:



Post a Followup:

Name:
E-Mail:

Subject:

Comments:

Optional Link URL:
Example: "http://www....html". Alternative write "http://www.ndt.net/wshop/attach/filename.htm" if you transfered a filename.htm via FTP
Page Title: is important!
Optional Image URL:
http://www....gif


Attention! Please click the button only once. This may take a moment to process


Forum General Discussions Help