Forum
General Discussions
Re: PCN vs. ASNT
Posted by: John O'Brien , E-mail: Address, on November 24, 2008 at 11:20 :In Reply to: PCN vs. ASNT posted by : Abdulla Benamer , E-mail: Address, on November 23, 2008 at 13:07 :
Abdullah
its not a great question as a good ASNT certified technician is just as good as a bad PCN certified technician.
The other issue is you are not distinguishing as to which form of ASNT you want to make a comparision with. ASNT SNT-TC-1A is an employer based certification and in some peoples eyes is therefore inferior to a third party issued certification such as PCN or the ASNT ACCP.
It also may vary dependent upon which discipline you wnat to employ MT & PT togeter with RT are relatively simple to compare. When you become more complex such as RT Film Interpretation or UT you may want to performance demonstration test all personnel and this takes out of the equation the certification. It then ensures the personnel you employ are truely capable.
- Re: PCN vs. ASNT S.Senthilkumar
16:46 Nov-30-2008 (7)
- Re: PCN vs. ASNT chris s
19:20 Dec-05-2008 (5)
- Re: PCN vs. ASNT Nigel Armstrong
12:57 Dec-06-2008 (4)
- Re: PCN vs. ASNT S.V.Swamy
15:07 Dec-06-2008 (2)
- Re: PCN vs. ASNT Oliviero Oldani
21:49 Dec-06-2008 (1)
- Re: PCN vs. ASNT Andre Fouche
07:03 Dec-07-2008 (0)
- Re: PCN vs. ASNT Dr D Dulay
![]()
14:06 Dec-06-2008 (0)
- Re: PCN vs. ASNT DDD 15:55 Dec-05-2008 (0)
- Re: PCN vs. ASNT Malik
00:18 Nov-28-2008 (1)
- Re: PCN vs. ASNT Thadakorn P.
00:12 Nov-29-2008 (0)
- Re: PCN vs. ASNT ASNT SNT-TC1A certified 09:34 Nov-25-2008 (2)
- Re: PCN vs. ASNT Nigel Armstrong
10:27 Nov-25-2008 (1)
- Re: PCN vs. ASNT Joe Buckley
![]()
21:39 Nov-25-2008 (0)