: Dear Sir.
: I would like to know which scheme i should accept when contractor doing job for me is it ASNT or PCN?
------------ End Original Message ------------Abdulla,
Needless to say, you only need a competent person to perform this task.I am holding duel certifiction both ASNT LEVEL3 and CSWIP level II as per EN 473 . I was not considered by some employers due to their policy but I always find excellent jobs, like my current position in ENIGAS.
So in my opinion, the employer shall screen the candidate based on his qualification and experience and shall conduct a 'real' test of the candiddate with mock up pieces( for example in case of UT) to test his current ability example API RP 2X...