Re: High temperature probes
Posted by: K. Matthies , E-mail: 6320vijayend@axp1.rz.bam-berlin.de, on October 04, 1996 at 12:38:34:In Reply to: High temperature probes posted by : Peter Hammond on September 24, 1996 at 17:13:46:
Dear Mr. Hammond,
The LNN piezo ceramic are developed in a project financed by EC research programme. In the same project, we have made further development in the transducer. The report that you find in the workshop is practically the final report.
It is true that these transducers are used in applications which requires large inspection time. We also use these transducers for determining wall thickness in Zinc coating plants. We measure the wall thickness by immersion technic in approximately 450 °C hot Zinc.
For your requirement, we have developed other type of transducers. As far as the construction of these transducers are concerned, it is similar to the previous one except that these are housed in plastic material. They are suitable only for continuous application up to 200 °C.
Since they posses ceramic delay path, it is possible to use these transducers on hot surfaces upto 1000 °C. However, this is possible in time intervals of 10 sec with 50 sec pause.