Investigation of Eddy Current Testing of Weld Zone by Uniform Eddy Current Probe

Kiyoshi KOYAMA , Hiroshi HOSHIKAWA and Noriyuki TANIYAMA
Nihon University
1-2-1 Izumicho Narashino Chiba 275-8575 , Japan
Tel : +81-47-474-2413 , Fax : +81-47-474-2399
Email : koyama@ee.cit.nihon-u.ac.jp
Contact

Abstract

INTRODUCTION

EDDY CURRENT TESTING OF WELD

EXPERIMENTAL SETUP

EXPERIMENTAL RESULTS

CONCLUSION

REFERENCES

  1. H.Hoshikawa and K.Koyama : "Eddy Current Testing by Uniform Eddy Current Probe" , Proceedings of 4th Far East Conference on NDT , pp43-52 (1997)
  2. H.Hoshikawa and K.Koyama : "Uniform Eddy Current Probe with Little Disrupting Noise" , Review of Progress in Quantitative Nondestructive Testing , Vol.17 , pp1059-1066 (1998)
  3. H.Hoshikawa and K.Koyama : "A New Eddy Current Probe using Uniform Rotating Eddy Current" , Materials Evaluation , Vol.56 , No.1 , pp85-89 (1998)
  4. H.Hoshikawa and K.Koyama : "Eddy Current Testing by Uniform eddy Current Probe", Proceeding of The 2nd Asian Joint Seminar on Applied Electromagnetics, pp1-6 (1998)
  5. H.Hoshikawa and K.Koyama : "Eddy Current Testing of Weld" , Proceeding of The 2nd Japan-US Symposium on Advances in NDT, pp232-235 (1999)

© AIPnD , created by NDT.net |Home|    |Top|