Conference & Proceedings

8th European Workshop On Structural Health Monitoring (EWSHM 2016)

5-8 July 2016, Spain, Bilbao
Right Now in Bilbao 17:42 Thu 13

Overview Program Right Now
Tue 5 Wed 6 Thu 7 Fri 8

105 Presentations during Tue 5 Jul

08:30-09:00 - A1
Opening Ceremony of EWSHM2016
09:00-09:30 - A1
Keynote: Design of Multifunctional Structural Batteries with Health Monitoring Capabilities.
Prof. Fu-Kuo Chang, Stanford University, USA
09:30-10:00 - A1
Keynote: Self-sufficient and self-contained sensing for local monitoring of in-situ bridge structures.
Prof. Hoon Soon, Korea Advanced Institute for Science and Technology (KAIST)
10:00-10:30 -
Coffee Break
New approaches
A1
Nathan Salowitz (Univ Wisconsin, USA), Francesc Pozo ( UPC, Spain)

10:30

Initial integration of structural health monitoring of self-healing materials

N. Salowitz*, P. Rohatgi, S. Suri, A. Correa

*Mechanical Engineering, University of Wisconsin - Milwaukee, Milwaukee, USA

10:50

Numerical Characterization of Mechanochromic Photonic Crystals for Structural Health Monitoring

V. Piccolo, A. Piotrowska, A. Chiappini, A. Chiappini, A. Vaccari, M. Ferrari, L. Deseri, D. Zonta*

*​Civil and Environmental Engineering, University of Strathclyde, Glasgow, United Kingdom

11:10

Electrical impedance tomography to monitor unsaturated moisture flows, and to detect corrosive elements and cracking in cementitious materials

A. Seppänen*, M. Hallaji, D. Smyl, M. Pour-Ghaz

*Department of Applied Physics, University of Eastern Finland, Kuopio, Finland

11:30

Contactless detachment identification in frescoes utilizing a Scanning Laser Doppler Vibrometer

C. Providakis*, M. Mousteraki, S. Tsistrakis, V. Liarakos

*School of Architecture, Technical University of Crete, CHANIA, Greece

11:50

Tensile Failure Analysis of Structural Materials using Acoustic Emission

J. Mowat**, S. Jihan, M. Droubi*

*Engineering, Robert Gordon University RGU, Aberdeen, United Kingdom

Guided waves modeling and simulations
A2
V. Giurgiutiu ( Univ South Carolina, USA), D. Saravanos (Univ Patras, Greece), R. Lammering ( HSU, Germany)

10:30

Predictive simulation of guided wave SHM with piezoelectric wafer active sensors

V. Giurgiutiu

UNIVERSITY OF SOUTH CAROLINA, Columbia, USA

10:50

Guided Wave-Gaussian Mixture Model based Damage Evaluation Method under Time-Varying Condition and Its Validation in a Full-Scale Aircraft Fatigue Test

L. Qiu*, S. Yuan, H. Mei, F. Fang

*The State Key Lab of Mechanics and Control of Mechanical Structures, Nanjing University of Aeronautics and Astronautics (NUAA), Nanjing, China

11:10

Guided Wave-based Damage Localization in Isotropic Structures with Smoothly Varying Thickness

J. Moll

Goethe-University Frankfurt am Main, Frankfurt am Main, Germany

11:30

Modified Time Reversal Imaging of Partially Closed Crack Based on Linear and Nonlinear Wave Response

P. Blanloeuil*, C. Wang, M. Veidt, F. Rose

*School of Mechanical & Mining Engineering, University of Queensland, Brisbane, Australia

11:50

Vibro-acoustic fault detection using a numerical time reversal method with reduced order models

S. Van Ophem*, E. Deckers, O. Atak, W. Desmet

*Mechanical Engineering, KU Leuven, Leuven, Belgium

12:10

Ultrasonic Techniques Based Inversion of Elastic Properties for a Single Lamina in Composites Laminates

J. Zhao*, J. Qiu, H. Ji

*Nanjing University of Aeronautics and Astronautics, State Key Laboratory of Mechanics and Control of Mechanical Structures, Nanjing, China

12:35-14:00 -
Lunch

14:00

Empirical technique for dispersion curve creation for guided wave applications

B. Hernandez-Crespo*, B. Engineer, C. Courtney

*The Welding Institute [TWI], Cambridge, United Kingdom

14:20

Numerical Simulation of the Cumulative Higher Harmonic Generation in Unidirectional Composites

N. Rauter*, R. Lammering

*Institute of Mechanics, Helmut-Schmidt-University / University of the Federal Armed Forces Hamburg (HSU), Hamburg, Germany

14:40

Investigation into Lamb wave boundary reflections in aluminium plates for defect characterisation and image reconstruction, with application to structural health monitoring.

A. Muller*, B. Robertson-Welsh, M. Gresil, P. Gaydecki, C. Soutis

*Faculty of Engineering and Physical Sciences, Aerospace Research Institute, The University of Manchester, Manchester, United Kingdom

15:00

Enhancement the estimation of damage severity by using guided wave diffraction resonance phenomena

E. Glushkov, N. Glushkova, A. Eremin*, R. Lammering

*Institute for Mathematics, Mechanics and Informatics, Kuban State University, Krasnodar, Russia

15:20

Wave Propagation Analysis in Composite Plates using a Novel Finite Wavelet Domain Method

D. Saravanos*, C. Nastos, T. Theodosiou, C. Rekatsinas

*Dept. of Mechanical Engineering and Aeronautics, University of Patras, Rion-Patras, Greece

15:40

Identification of Impact Events on Composite Plates using Wave Characteristics and Impact Similarity Models

D. Saravanos*, T. Theodosiou, C. Rekatsinas, C. Nastos, M. Iglesias Vallejo, J. Garcia Alonso

*Dept. of Mechanical Engineering and Aeronautics, University of Patras, Rion-Patras, Greece

16:00-16:30 -
POSTERS-1 (Coffee & Drinks will be served)

16:30

Assessment of correlation-based imaging technique on composites

P. Ostiguy*, N. Quaegebeur, P. Masson

*Université de Sherbrooke, Sherbrooke, Canada

16:50

Numerical Study of Rayleigh Wave Based Interfacial Debonding Detection between FRP Plate and Steel Beam

Y. Xu*, B. Li

*Harbin Institute of Technology Shenzhen Graduate School, Shenzhen, China

Fiber Optic Sensors Systems
A3A
M. Tur (Tel-Aviv Univ., Israel), P. Ferdinand (CEA, France), M. Giordano ( Univ Sannio, Italy)

10:30

INVITED PAPER: Overview of Rayleigh-Based High Definition Distributed Fiber Optic Sensing for Structural Testing and Health Monitoring Applications

B. Soller

Luna Innovations, Blacksburg, USA

10:50

Demonstration and methodology of structural monitoring of hidden composite areas by embedded optical fiber sensors and connectors

C. Miguel Giraldo*, J. Zúñiga Sagredo, L. Garcia Vazquez, J. Cardenas Aguado

*Materials & Processes, Airbus Operations, Madrid, Spain

11:10

A Numerical Study for Damage Detection of a Thin Plate Using Macro-Strain Measurement

T. Hsu*, W. Liao, Y. Shi

*National Center of Research on Earthquake Engineering (NCREE), Taipei,

11:30

Parameter identification based on quasi-continuous strain data captured by high resolution fiber optic sensing

A. Künzel*, Y. Petryna

*Chair of Structural Mechanics, Technische Universität Berlin (TU Berlin), Berlin, Germany

11:50

Fiber optic based HUMS concept for large aircraft structure based on both point and distributed strain sensing

I. Kressel*, M. Tur**, M. Bosboom, R. Evenblij, P. Michaelides, U. Ben-Simon, N. Gorbatov, A. Bergman, N. Kontis, C. Koimtzoglou

*Israel Aerospace Industries (IAI), Tel Aviv, Israel

12:10

Fiber Optic Based In-Flight Structural Health Monitoring (SHM) Implemented on a Gearbox Support Beam of a Helicopter

O. Shapira*, S. Shoham, U. Ben-Simon, N. Gorbatov, B. Glam, V. Kalmanovich, T. Yehoshua, I. Kressel**, M. Tur

*Technion Institute of Technology, Haifa, Israel

12:35-14:00 -
Lunch

14:00

Properties of optical fibers and FBG sensors and strain monitoring of the composite structures

M. Ruzicka*, M. Dvorak

*Dpt. of mechanics, biomechanics and mechatronics, Czech Technical University in Prague, Fac. of Mech. Eng., Praha 4, Czech Republic

14:20

Bond strength and performance of optical fibre Bragg Grating sensors embedded in composite patch repairs for military aircrafts

T. Jones**, T. Thorvaldsen*, G. Sagvolden, K. Pran, T. Olsen

*Land Systems Division, Norwegian Defence Research Establishment (FFI), Kjeller, Norway

14:40

Robust integration of optical fiber sensors for aerospace applications in composite material structures

M. Frövel*, J. Pintado, G. Carrión, F. Cabrerizo, F. Terroba, T. Buck, A. Reutlinger, J. San Millán

*Composite Materials, Spanish Institue for Aerospace Technology (INTA), Torrejón de Ardoz, Spain

15:00

Fiber Optic Sensors for Multiparameter Monitoring Of Large Scale Assets

D. Karabacak*, M. Farnan, S. Ibrahim, M. Todd, J. Singer

*Fugro Technology B.V., Leidschendam, Netherlands

15:20

Local Strain Monitoring of Fiber Reinforced Composites under High Strain Fatigue using Embedded FBG Sensors

A. Suleman*, E. Kocaman, E. Akay, C. Yilmaz, H. Turkmen, I. Misirlioglu, M. Yildiz

*Mechanical Engineering, University of Victoria, Victoria, Canada

15:40

Application of Biaxial FBG Sensors to Monitor Poisson’s Ratio of Composites as Damage Index

A. Suleman*, C. Yilmaz, C. Akalin, E. Kocaman, M. Yildiz

*Mechanical Engineering, University of Victoria, Victoria, Canada

16:00-16:30 -
POSTERS-1 (Coffee & Drinks will be served)

16:30

Investigation of the performance in dynamic strain measurements of distributed fiber optic sensors

H. Murayama*, K. Kageyama, T. Matsuo, T. Tamaoki, F. Fujimori, K. Shiotsubo, D. Wada, H. Igawa

*School of Engineering, The University of Tokyo, Tokyo, Japan

16:50

A curvature based approach in dynamic monitoring using long-gage fiber optic sensors

K. Kliewer*, B. Glisic

*Civil and Environmental Engineering, Princeton University, Princeton, USA

17:10

Fibre optic sensors structural health monitoring of the central beam pipe in the CMS experiment at the CERN laboratories

F. Fienga*, G. Breglio, S. Buontempo, Z. Szillasi, N. Beni, A. Gaddi, A. Gaddi, A. Cusano, M. Consales, M. Giordano

*Department of Information Technology and Electrical Engineering (DIETI), University of Naples Federico II (UNINA), Napoli, Italy

17:30

Assessment of a multicore optical fibre interferometer for strain sensing in aerospace structures

O. Arrizabalaga*, J. Villatoro, G. Durana, I. García, A. Montero, E. Antonio-Lopez, A. Schülzgen, R. Amezcua Correa, J. Zubia, I. Sáez de Ocáriz

*University of the Basque Country (UPV/EHU), BILBAO, Spain

17:50

Model-assisted performance qualification of a distributed SHM system for fatigue crack detection on a helicopter tail boom

C. Sbarufatti*, M. Corbetta, J. San Millán, M. Frövel, M. Stefaniuk, M. Giglio

*Department of Mechanical Engineering, Politecnico di Milano, Milano, Italy

18:10

Ultrasonic strain wave acquisition by a low-cost fiber optic coherent sensor for structural health monitoring applications

C. Sbarufatti*, L. Martinelli, M. Mattarei, M. Ferrario, M. Giglio

*Department of Mechanical Engineering, Politecnico di Milano, Milano, Italy

18:30

Free-edge delamination location and growth montoring with an embedded distributed fiber optic network

P. Fernández Díaz-Maroto*, A. Fernández López, A. Güemes, B. Larrañaga

*Center of Composite Materials and Smart Structures, Polytechnical University of Madrid (UPM), Madrid, Spain

Image processing
A3B
G Akhras (Royal Military College, Canada)

10:30

Defect triangulation via demixing algorithms based on dictionaries with different morphological complexity

J. Druce, S. Gonella*, M. Kadkhodaie, S. Jain, J. Haupt

*Civil, Environmental, and Geo-Engineering, University of Minnesota, Minneapolis, USA

10:50

Heat transfer 1D modeling for Non Destructive Testing and Structural Health Monitoring for civil engineering structures improved by GPGPU

A. Crinière*, J. Dumoulin, L. Mevel

*I4S Team, Inria, Rennes, France

11:10

Automatic crack detection on pressed panels using camera image processing

C. Lee*, H. Jung, G. Park

*Mechanical engineering, chonnam national university, Gwangju, South Korea

11:30

dynamic displacement measurement of a long-span bridge using vision-based system

Y. Xu*, J. Brownjohn, D. Hester, K. Koo

*College of Engineering, Mathematics and Physical Sciences, university of exeter, Exeter, United Kingdom

11:50

Noncontact 3D measurement system for furnace wall maintenance support

M. Ryu*, H. Sakamoto, Y. Ohbuchi, E. Nakamachi, Y. Nakamura, T. Yoshida

*Graduate School of Engineering and Technology, Kumamoto University, Kumamoto, Japan

12:10

Vision-based multi-point displacement measurement for SHM

D. Feng*, M. Feng**

*Columbia University, New York, USA

12:35-14:00 -
Lunch
Optimization sensors topology
A3B
J. Rodellar (UPC, Spain), N. Constantin ( UPB, Romania)

14:00

Optimal Frequency selection for vibration based damage detection using pattern recognition

D. Hesser*, B. Markert

*Institute of General Mechanics, RWTH Aachen University, Aachen, Germany

14:20

Characterization of the robustness of SHM imaging techniques using the absolute error of localization

J. Moriot*, N. Quaegebeur, A. Le Duff, P. Masson

*Dpt. Of Mechanical Engineering, Groupe d\'Acoustique de l\'Université de Sherbrooke, Sherbrooke, Canada

14:40

Sensor Placement for Modal Parameter Subset Estimation: A Frequency Response-based Approach

M. Ulriksen*, D. Bernal, L. Damkilde**

*Aalborg University, Esbjerg, Denmark

15:00

A Linearized Impact Localisation Algorithm for the Health Monitoring of Aerospace Components

M. De Simone, S. Boccardi, F. Ciampa*, M. Meo

*University of Bath, Bath, United Kingdom

16:00-16:30 -
POSTERS-1 (Coffee & Drinks will be served)
SHM for Oil & Gas industries
A3B
Dr. Michel Leblanc(Halliburton, USA), J. Singer ( Fugro Technologies, Netherlands)

16:30

A FIBEROPTIC SENSING SYSTEM FOR SYSTEM HEALTH MONITORING IN OIL&GAS INDUSTRY APPLICATIONS

J. Singer*, D. Karabacak**, M. Farnan, S. Ibrahim, M. Todd

*Fugro Technology BV, Leidschendam, Netherlands

16:50

Multidimensional big data processing for damage detection in real pipelines using a smart pig tool

M. Ruiz*, L. Mujica, M. Quintero, R. Villamizar, S. Alférez

*Department of Mathematics, Escola d’Enginyeria de Barcelona Est (EEBest),Campus Diagonal-Besós, Universitat Politécnica de Catalunya (UPC), Barcelona, Spain

17:10

study on in-situ capacitive sensor for monitoring engine lubricant oil debris

Y. Wang*, Z. Han, D. Liang, X. Qing**

*School of Aerospace Engineering, Xiamen University (XMU), Xiamen, China

17:30

Distributed Fiber Optic Fuel Leak Detection System

E. Mendoza

Redondo Optics Inc, Redondo Beach, USA

17:50

Towards a condition monitoring scheme for combustion instability detection and fuel blends performance classification in gas turbine engines using pattern recognition and advanced machine learning

I. Matthaiou*, B. Khandelwal, I. Antoniadou

*Dynamics Research Group, Department of Mechanical Engineering, University of Sheffield, Sheffield, United Kingdom

18:10

Experimental study of ultrasound characteristics in steel samples cut out of a pipeline that has been exploited during a long time

A. Malkhanov*, V. Erofeev

*Mechanics Engineering Research Institute, Russian Academy of Sciences, Nizhny Novgorod, Russia

Concrete
A4
K. Loh (UCSD, USA)

10:30

Pre- and post- damage structural health monitoring in carbon fiber textile reinforced concrete (TRC) structures

Y. Goldfeld*, T. Quadflieg, T. Gries

*Faculty of Civil and Environmental Engineering, Technion - Israel Institute of Technology, Haifa, Israel

10:50

Recognition of Rebar and Crack Based on Impact-Echo Phase Analysis

P. Liu, P. Yeh, L. Lin, Y. Hsu*, C. Yeh

*National Taiwan University, NTU, Taipei,

11:10

Narrow-band diffuse ultrasonic wave field measurements in a network of reciprocal transducers for monitoring of a large concrete floor slab

P. Fröjd*, P. Ulriksen

*Engineering Geology, Lund University, Lund, Sweden

11:30

Moisture in screed: a non-destructive multi-sensor approach

C. Strangfeld*, S. Kruschwitz, J. Wöstmann, S. Nagel, F. Hase

*8.2 Non-Destructive Damage Assessment and Environmental Measurement Methods, Bundesanstalt für Materialforschung und -prüfung, Berlin, Germany

11:50

The sensitivity of coda wave interferometry in different scattering regimes

P. Fröjd*, P. Ulriksen

*Engineering Geology, Lund University, Lund, Sweden

12:35-14:00 -
Lunch

14:00

Moisture measurements with RFID based sensors in screed and concrete

C. Strangfeld*, S. Johann, M. Müller, M. Bartholmai

*8.2 Non-Destructive Damage Assessment and Environmental Measurement Methods, Bundesanstalt für Materialforschung und -prüfung, Berlin, Germany

14:20

The use of electromechanical impedance based structural health monitoring technique in concrete structures

R. Silva, K. Tsuruta*, D. Rabelo, R. Finzi Neto, V. Steffen Jr.

*School of Mechanical Engineering, FEDERAL UNIVERSITY OF UBERLÂNDIA (UFU), UBERLÂNDIA, Brazil

14:40

Design of Embedded Piezoelectric Transducers for Structural Health Monitoring in concrete structures.

C. Dumoulin*, A. Deraemaeker

*Building, Architecture and Town Planning (BATir), Université Libre de Bruxelles (ULB), Brussels, Belgium

15:00

Active Structural Health Monitoring of Reinforced Concrete Structures using Piezoelectric Smart Aggregates

T. Nestorovic*, D. Stojic, N. Markovic

*Mechanics of Adaptive Systems, Ruhr University Bochum, Bochum, Germany

15:20

Monitoring of Unsaturated Moisture Flow in Cement-based Materials with Electrical Capacitance Tomography

A. Voss*, M. Pour-Ghaz, M. Vauhkonen, A. Seppänen

*Department of Applied Physics, University of Eastern Finland (UEF), Kuopio, Finland

15:40

Thermal imaging coupled with high-definition colour imaging for defect localisation and quantification

B. Guldur

Department of Civil Engineering, Hacettepe University, Ankara, Turkey

16:00-16:30 -
POSTERS-1 (Coffee & Drinks will be served)
Civil Structures. Modeling, experimental demonstrations
A4
W. Habel (BAM Berlin, Germany), J Lynch (Univ. Michigan, USA), D. Inaudi (Smartec, Switzerland)

16:30

A methodology for dam safety evaluation and anomaly detection based on boosted regression trees

F. Salazar*, J. González, M. Toledo, E. Oñate

*International Center for Numerical Methods in Engineering (CIMNE), Madrid, Spain

16:50

Implementation of communication, collection and tracking units in crisis operation

F. Casciati, S. Casciati, L. Faravelli, M. Vece*

*DICAr, University of Pavia, Pavia, Italy

17:10

Assessment of the structural behaviour of concrete dams based on wavelet transforms

J. Caires da Mata*, J. Santos

*Concrete Dam Department, Portuguese National Laboratory for Civil Engineering (LNEC), Lisbon, Portugal

17:30

A Diverse Monitoring for Post-Accident using Alternative Powers

J. Kim

I&CHumanFactor Division, Korea Atomic Energy Research Institute, Daejeon, South Korea

17:50

Debonding identification of FRP strengthened concrete beams with PZT sensors

R. Perera*, R. Sun, E. Sevillano, M. Baena, C. Barris

*Mechanical Engineering, Technical University of Madrid (Spain), Madrid, Spain

18:10

Review of Distributed Optical Fiber Sensors in Civil Engineering applications

A. Barrias*, J. Casas, S. Herrero

*Department of Civil and Environmental Engineering, Technical University of Catalonia . Barcelonatech (UPC), Barcelona, Spain

18:30

The static and dynamic monitoring of the Asinelli Tower in Bologna,Italy

S. Baraccani*, M. Palermo**, S. Silvestri, G. Gasparini, T. Trombetti, R. Azzara

*University of Bologna, Bologna, Italy

Damage detection by Acoustic Emission
B1
L. Faravelli ( Univ Pavia, Italy), M. Gresil ( Manchester Univ., UK)

10:30

Defect quantification in 3D Angle Interlock Glass Fibre Composites using Acoustic Emission

M. Gresil*, M. Saleh, M. Arshad, C. Soutis

*University of Manchester, Manchester, United Kingdom

10:50

Identification of diagnostic and prognostic features by means of AE and hydraulic pressure measurements

N. Beganovic*, S. Rothe, D. Söffker

*Chair of Dynamics and Control, University of Duisburg-Essen, Duisburg, Germany

11:10

Impact Damage Assessment of Multi-Layered Composite Structures in Service by Acoustic Emission Source Location Analysis

D. Yoon*, B. Han, I. Kim, C. Park, I. Kwon

*Korea Research Institute of Standards and Science (KRISS), Daejeon, South Korea

11:30

Experimental results of frequency-based classification of damages in composites

S. Wirtz*, N. Beganovic, D. Söffker

*University of Duisburg-Essen, Chair of Dynamics and Control, Duisburg, Germany

11:50

Guided wave propagation modelling to aid understanding of acoustic emission system performance on complex aerospace structures

M. Courtier*, A. Croxford, K. Atherton

*Mechanical Engineering, University of Bristol, Bristol, United Kingdom

12:10

New methods for onset detection of acoustic emission signals

D. Gagar*, F. Bai, Y. Zhao, P. Foote

*School of Aerospace, Transport and Manufacturing, Cranfield University, Cranfield, United Kingdom

12:35-14:00 -
Lunch
Uncertainty. Statistical Methods for SHM.
B1
S. Fassois (Univ Patras, Greece), Lea Cot (Inst Clement Ader, France), D. Zonta (Univ Trento, Italy)

14:00

Uncertainties when using EVA (extreme value analysis) in SHM

F. Cegla*, D. Benstock

*Mechanical Engineering, Imperial College London, London, United Kingdom

14:20

Evaluation of the probability of failure using Bayesian theorem for real-time condition monitoring

A. Iwasaki*, Y. Sanyoshi

*Gunma University, Gunma, Japan

14:40

Comprehensive Bayesian structural identification applied to a scale aluminium bridge

A. Jesus*, Y. Zhu, I. Laory

*School of Engineering, University of Warwick, Coventry, United Kingdom

15:00

Statistical Damage Localization with Stochastic Load Vectors Using Multiple Mode Sets

M. Bhuyan*, M. Döhler, L. Mevel

*I4S Team, Institut national de recherche en informatique et en automatique (INRIA), Rennes, France

15:20

Statistical Impact-echo Analysis using Bag-of-echoes Model for Concrete Condition Assessment

J. Ye*, T. Kobayashi, M. Iwata, M. Murakawa

*Artificial Intelligence Applications Research Team, National Institute of Advanced Industrial Science and Technology (AIST), Tsukuba, Japan

15:40

Damage Detection of Structures with Detrended Fluctuation and Detrended Cross-Correlation Analyses

H. Fajri, M. Wang, T. Lin*

*Civil Engineering, National Chiao Tung University, Hsin-Chu,

16:00-16:30 -
POSTERS-1 (Coffee & Drinks will be served)

16:30

GPGPU implementation of modal parameter tracking by particle based Kalman filter

A. Crinière*, L. Mevel, J. Dumoulin, M. Zghal

*I4S Team, Inria, Rennes, France

16:50

Applying Extreme Value Theory for alarm and warning levels setting under variable operating conditions

D. Filcheva*, N. Lieven, P. Morrish, P. Hutchinson

*University of Bristol, Bristol, United Kingdom

17:10

A structural damage detection technique based on agglomerative clustering applied to the Z-24 Bridge

M. Silva*, A. Santos, R. Santos, E. Figueiredo**, C. Sales, J. Costa

*Applied Electromagnetism Laboratory, Federal University of Pará, Belém, Brazil

17:30

Solving Bayesian multi-parameter estimation problems using the mechanical equivalent of logical inference

D. Bolognani*, C. Cappello, D. Zonta**

*Deptartment of Civil, Environmental and Mechanical Engineering, University of Trento, Trento, Italy

Piezoelectrics as sensors/actuators
C1
Vincent Le Cam (IFSTTAR, F), Luca de Marchi (Univ. Bologna, IT), Tadeusz Uhl (AGH Univ., Poland)

10:30

A design strategy for highly directional piezoelectric transducers for Lamb waves inspections

L. De Marchi*, N. Testoni, A. Marzani

*University of Bologna, Bologna, Italy

10:50

A stamp size, 40mA, 5 grams sensor node for impact detection and location

N. Testoni*, L. De Marchi, A. Marzani

*Department of Electrical, Electronic, and Information Engineering \, University of Bologna, Bologna, Italy

11:10

Influence of delamination and temperature conditions on electromechanical impedance

P. Malinowski*, T. Wandowski, W. Ostachowicz

*Institute of Fluid-Flow Machinery, Polish Academy of Sciences, Gdansk, Poland

11:30

A novel self-tuning method for Lamb wave inspection of plate-like structures

A. Dominguez-Macaya*, J. Romero, J. Vicente, J. Vicente, A. Iturrospe, J. Abete, F. Martin De La Escalera, A. Alcaide

*Mondragon University-Faculty of Engineering (MGEP), Arrasate, Spain

11:50

A semi-analytical approach to design of a transducer for selective wave generation

P. Packo*, M. Gawronski**, M. Miszczynski, P. Zbyrad, T. Stepinski, J. Lis, T. Uhl

*Department of Robotics and Mechatronics, AGH - University of Science and Technology, Krakow, Poland

12:10

SHM of Thick Structures via E/M Impedance of Embedded PWAS for Weight Loss Defects

T. Kamas*, T. Kamas*, M. Tekkalmaz

*Eskisehir Osmangazi University, Eskisehir, Turkey

12:35-14:00 -
Lunch

14:00

Piezo-electric Thick Films for Sensing

M. Eaton*, J. Hale, M. Pearson, D. Crivelli, A. Deligianni

*Cardiff School of Engineering, Cardiff University, Cardiff, United Kingdom

14:20

Optimization of Energy Harvesting concepts from vibration by piezoelectric actuator design.

N. Murillo*, J. Maudes, A. Pérez Márquez, J. Ortiz, G. Aranguren

*Trasnport & Industry Division, TECNALIA, Donostia-San Sebastian, Spain

14:40

About the Effects of Debonding of PWAS on the Wave Propagation and the Electro-Mechanical Impedance Spectrum

I. Mueller*, A. Shpak, M. Golub, C. Fritzen**

*Department of Mechanical Engineering, University of Siegen, Siegen, Germany

15:00

Impact Detection System for Structures during their Storage and Transport

G. Aranguren*, J. Ortiz**, J. Etxaniz, N. Murillo, J. Maudes, A. Donado, E. Rueda, A. Pérez Márquez

*Electronic technology, University of the Basque Country (UPV/EHU), Bilbao, Spain

16:00-16:30 -
POSTERS-1 (Coffee & Drinks will be served)
Sensors other than PZT and FOS
C1
F. Casciati ( Univ Pavia, Italy)

16:30

Investigating the performance of OEM devices for structural monitoring

F. Casciati*, S. Casciati, L. Faravelli, M. Vece

*University of Pavia, Pavia, Italy

16:50

SHM with EMATs

F. Cegla*, J. Isla-Garcia, B. Herdovics

*Mechanical Engineering, Imperial College London, London, United Kingdom

17:10

Response comparison of FBG sensor, strain gage, and piezo-electric accelerometer in an aluminum cantilever beam shock load

S. Fukumoto*, N. Tomio

*Technical Research & Development Center, IHI Inspection & Instrumentation Co., Ltd., Yokohama, Japan

17:30

Radar-based Mechanical Vibration Sensing for Structural Health Monitoring Applications: A Comparison of Radar Transceiver Measurements at 24GHz and 100GHz

J. Moll*, V. Krozer

*Goethe-University Frankfurt am Main, Frankfurt am Main, Germany

18:10

GNSS and multi-sensor fusion technique applied to an experimental model

R. Seabra*, S. Magalhaes, C. Felix, C. Rodrigues

*Construct-FEUP, Faculty of Engineering of University of Porto, Porto, Portugal