Wave Propagation Analysis in Composite Plates using a Novel Finite Wavelet Domain Method

Abstract »
Paper

Authors

Saravanos, Dimitris A*Nastos, Christos VTheodosiou, Theodosis CRekatsinas, Christoforos S*Contact