Additive manufacturing for novel structural health monitoring systems

Abstract »
Paper

Authors

Strantza, Maria*Hinderdael, MichaelDe Baere, DieterVandendael, IsabelleTerryn, HermanVan Hemelrijck, DannyGuillaume, Patrick*Contact