Steel - Rubber debond testing method?

I am looking for a methodology that is capable of detecting bonding/adhesive failures between a rubber type compound and heavy steel plating, and determine if off-the-shelf testing equipment is available.
The steel-side surface is mostly inaccessible. Testing must either be done from the rubber surface, or from very limited locations on the steel-side surface.
The rubber compound is approximately 2" thick and cannot be penetrated by ultrasound, at any frequency.
Critical size of debond has not been determined.

Thank you,
B Johnson
NDT Engineering
General Dynamics, Electric Boat


 
 Reply 
 
joerg collrep
Director, - Sales NDT
Dantec Dynamics GmbH, Germany, Joined Jan 2006, 4

joerg collrep

Director, - Sales NDT
Dantec Dynamics GmbH,
Germany,
Joined Jan 2006
4
08:32 Apr-05-2007
Re: Steel - Rubber debond testing method?
you should try shearography which has proved to detect easily voids inside rubber. we load your part with vacuum and the defect expands to the surface. if you need more info pls let me know or visit our homepage. best regards joerg----------- Start Original Message -----------
: I am looking for a methodology that is capable of detecting bonding/adhesive failures between a rubber type compound and heavy steel plating, and determine if off-the-shelf testing equipment is available.
: The steel-side surface is mostly inaccessible. Testing must either be done from the rubber surface, or from very limited locations on the steel-side surface.
: The rubber compound is approximately 2" thick and cannot be penetrated by ultrasound, at any frequency.
: Critical size of debond has not been determined.
: Thank you,
: B Johnson
: NDT Engineering
: General Dynamics, Electric Boat
------------ End Original Message ------------




 
 Reply 
 
Tom Nelligan
Engineering,
retired, USA, Joined Nov 1998, 390

Tom Nelligan

Engineering,
retired,
USA,
Joined Nov 1998
390
01:14 Apr-05-2007
Re: Steel - Rubber debond testing method?
In other situations where the rubber is thinner and more transmissive to ultrasound, we usually recommend a phase shift test using any common flaw detector and an appropriate transducer, but you indicate that won't work here due to extreme attenuation. Alternately, if testing from the points where you do have access to the steel is useful, it should be possible to evaluate the steel/rubber bond from the steel side using the ringdown technique described in the attached application note.

----------- Start Original Message -----------
: I am looking for a methodology that is capable of detecting bonding/adhesive failures between a rubber type compound and heavy steel plating, and determine if off-the-shelf testing equipment is available.
: The steel-side surface is mostly inaccessible. Testing must either be done from the rubber surface, or from very limited locations on the steel-side surface.
: The rubber compound is approximately 2" thick and cannot be penetrated by ultrasound, at any frequency.
: Critical size of debond has not been determined.
: Thank you,
: B Johnson
: NDT Engineering
: General Dynamics, Electric Boat
------------ End Original Message ------------




 
 Reply 
 
Thomas F. Murphy
Thomas F. Murphy
07:15 Apr-06-2007
Re: Steel - Rubber debond testing method?
Hello all,

My employer, GE Inspection has a system used for this application in rubber covered rolls. It operates by the principle of heating the metal from the rubber, inductively, and monitoring the transferred heat to the rubber. Lack of thermal transfer indicates a lack of bond. If you are interested in it I will give you the correct contacts for further information.

Kind regards all,
Tom

Kindest regards,
Tom




 
 Reply 
 
Trevor Easton
Engineering
Dofasco Inc, Canada, Joined Nov 1998, 13

Trevor Easton

Engineering
Dofasco Inc,
Canada,
Joined Nov 1998
13
04:53 Apr-13-2007
Re: Steel - Rubber debond testing method?
You might try a sub sonic method. Determine the natural frequency of a bonded portion of the rubber using a shaker. Then measure the natural frequency of a debonded portion. If there is a significant difference then a scan of the surface to measure the frequency response will provide an indication of debonding. You will of course have to develop your own transducer but it shouldn't be to difficult to adapt a small electric motor with offset mass and an accelerometer into a simple hand held monitor. Maybe a roller ball to ease the job of scanning across large areas. Perhaps an electro magnet driven at the appropriate frequency(s) the variation in its behaviour over bonded and unbonded rubber indicating areas of concern.

----------- Start Original Message -----------
: I am looking for a methodology that is capable of detecting bonding/adhesive failures between a rubber type compound and heavy steel plating, and determine if off-the-shelf testing equipment is available.
: The steel-side surface is mostly inaccessible. Testing must either be done from the rubber surface, or from very limited locations on the steel-side surface.
: The rubber compound is approximately 2" thick and cannot be penetrated by ultrasound, at any frequency.
: Critical size of debond has not been determined.
: Thank you,
: B Johnson
: NDT Engineering
: General Dynamics, Electric Boat
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

Panther

M2M PANTHER is a phased-array equipment designed for both desktop and industrial applications, offer
...
ing unparalleled performance in a compact unit. It combines the speed required for industrial integrated Phased-Array Ultrasound (PAUT) solutions, with the most complete set of total focusing method (TFM) imaging techniques, making it the ultimate tool for R&D and procedure qualification.
>

Navic - Steerable Modular Automated Scanner

The Navic is a modular, motorized, steerable scanner designed to carry multiple attachments used
...
in various scanning and inspection applications. The Navic is capable of weld scanning (girth welds and long seam welds), automated corrosion mapping, and tank scanning.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

Semi-Automated Phased Array Immersion System for Small Composite Parts

Turn-key semi-automated system as an improved and affordable solution for inspection of small comp
...
osite parts. Includes support table, immersion tank, scanner, PA instrument, PC, Analysis software, database, wedge management and other options.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window