Nguyen Thanh Chung
Nguyen Thanh Chung
03:25 May-25-2007
NDT for automotive parts

Dear Alls,

We are a company specialized in manufaturing of connecting rods for motorbike engines with products capacity is 5000 products per day. 100% of our products need to be NDT check for surface flaws with inspection rate upto 600 products per hour. Please advice us what method and equipment can handle this task.

Thanks you,



 
 Reply 
 
Nigel
Engineering, - Specialist services
United Kingdom, Joined Oct 2000, 1096

Nigel

Engineering, - Specialist services
United Kingdom,
Joined Oct 2000
1096
07:00 May-26-2007
Re: NDT for automotive parts

Magnetic Analysis Corporation have many different system for rapid screening of machined parts for surface defects.

www.mac-ndt.com

Regards

----------- Start Original Message -----------
: Dear Alls,

: We are a company specialized in manufaturing of connecting rods for motorbike engines with products capacity is 5000 products per day. 100% of our products need to be NDT check for surface flaws with inspection rate upto 600 products per hour. Please advice us what method and equipment can handle this task.
: Thanks you,
------------ End Original Message ------------




 
 Reply 
 
Amiri
Consultant, NDT/QC/WELD INSPECTION
Iran, Joined Nov 2005, 20

Amiri

Consultant, NDT/QC/WELD INSPECTION
Iran,
Joined Nov 2005
20
01:36 May-26-2007
Re: NDT for automotive parts
Dear Friend,
Refering to your inquiry,for automative long parts,MT by bench unit is prefered.you should select type of techniques(magnetic field type)in accordance with important defects orientation and direction.multi directional system with wet bath fluorescent is prefered.

----------- Start Original Message -----------
: Dear Alls,
: We are a company specialized in manufaturing of connecting rods for motorbike engines with products capacity is 5000 products per day. 100% of our products need to be NDT check for surface flaws with inspection rate upto 600 products per hour. Please advice us what method and equipment can handle this task.
: Thanks you,
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Lyft™: Pulsed Eddy Current Reinvented

PEC Reinvented—CUI Programs Redefined Corrosion under insulation (CUI) is possibly the greatest u
...
nresolved asset integrity problem in the industry. Current methods for measuring wall thickness with liftoff, without removing insulation, all have severe limitations. Eddyfi introduces Lyft — a reinvented, high-performance pulsed eddy current (PEC) solution. The patent- pending system features a state-of-the-art portable instrument, real- time C-scan imaging, fast data acquisition with grid-mapping and dynamic scanning modes, and flexibility with long cables. It can also scan through thick metal and insulation, as well as aluminum, stainless steel, and galvanized steel weather jackets. Who else but Eddyfi to reinvent an eddy current technique and redefine CUI programs. Got Lyft?
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window