01:47 Jul-20-2000
backing load

My name is Simone Brocco, I'm an Italian student in his final year in Biomedical Engineering- "La Sapienza" University in Rome (Italy).
I'm working on my thesis concerning Ultrasonic Transducers for Noninvasive Medical Application: probe (backing load,bonding layer,PZT,matching layers and acousticFor my thesis I'm now verifying the correspondence between the texts on the argument and the effective realization by constructors. I'm analiyzing a Toshiba's probe (you can see it in the file enclosed, called probe ). By a SEM (Scanning Electron Microscopy) analysis the composition of the backing material has resulted (weight percent):
Cl=40
Si=1.27
S=9.48
K=18.39
Ca=4.36
Fe=6.68
Pb=17
Ti=2.58
What kind of backing material is? (i.e. tungsten/epoxy...)
On the rear face of the backing there is a circular blind hole (you can see it in the file enclosed, called blind hole ). What's its use?
Dividing the backing and the electric circuitation there is an air layer. why? May be an insulating or an ulterior backing layer?
Moreover, on the rear face of a different probe at the end of the backing there is a glass plate bonded.What's its use?

Thank you very much for your attention

Simone Brocco
al lens).


 
 Reply 
 
Dipl.-Ing. Martin Heinz
Dipl.-Ing. Martin Heinz
00:22 Jul-20-2000
Re: backing load
: My name is Simone Brocco, I'm an Italian student in his final year in Biomedical Engineering- "La Sapienza" University in Rome (Italy).
: I'm working on my thesis concerning Ultrasonic Transducers for Noninvasive Medical Application: probe (backing load,bonding layer,PZT,matching layers and acousticFor my thesis I'm now verifying the correspondence between the texts on the argument and the effective realization by constructors. I'm analiyzing a Toshiba's probe (you can see it in the file enclosed, called probe ). By a SEM (Scanning Electron Microscopy) analysis the composition of the backing material has resulted (weight percent):
: Cl=40
: Si=1.27
: S=9.48
: K=18.39
: Ca=4.36
: Fe=6.68
: Pb=17
: Ti=2.58
: What kind of backing material is? (i.e. tungsten/epoxy...)
: On the rear face of the backing there is a circular blind hole (you can see it in the file enclosed, called blind hole ). What's its use?
: Dividing the backing and the electric circuitation there is an air layer. why? May be an insulating or an ulterior backing layer?
: Moreover, on the rear face of a different probe at the end of the backing there is a glass plate bonded.What's its use?
:
: Thank you very much for your attention
:
: Simone Brocco
: al lens).
Dear Mr. Brocco,

unfortunately your file which should be enclosed is not attached. Could you specify a web page where I can download the file? Or could you send it directly to my email adress heinz@ibmt.fhg.de ?

Best regards,

Martin Heinz.



 
 Reply 
 
harish tikadia
harish tikadia
08:27 Nov-15-2001
Re: backing load
: : My name is Simone Brocco, I'm an Italian student in his final year in Biomedical Engineering- "La Sapienza" University in Rome (Italy).
: : I'm working on my thesis concerning Ultrasonic Transducers for Noninvasive Medical Application: probe (backing load,bonding layer,PZT,matching layers and acousticFor my thesis I'm now verifying the correspondence between the texts on the argument and the effective realization by constructors. I'm analiyzing a Toshiba's probe (you can see it in the file enclosed, called probe ). By a SEM (Scanning Electron Microscopy) analysis the composition of the backing material has resulted (weight percent):
: : Cl=40
: : Si=1.27
: : S=9.48
: : K=18.39
: : Ca=4.36
: : Fe=6.68
: : Pb=17
: : Ti=2.58
: : What kind of backing material is? (i.e. tungsten/epoxy...)
: : On the rear face of the backing there is a circular blind hole (you can see it in the file enclosed, called blind hole ). What's its use?
: : Dividing the backing and the electric circuitation there is an air layer. why? May be an insulating or an ulterior backing layer?
: : Moreover, on the rear face of a different probe at the end of the backing there is a glass plate bonded.What's its use?
: :
: : Thank you very much for your attention
: :
: : Simone Brocco
: : al lens).
: Dear Mr. Brocco,

: unfortunately your file which should be enclosed is not attached. Could you specify a web page where I can download the file? Or could you send it directly to my email adress heinz@ibmt.fhg.de ?

: Best regards,

: Martin Heinz.

followed by harish


 
 Reply 
 

Product Spotlight

NDT Master Lecturer

In the program both university professors and practitioners will give lectures, which guarantees the
...
oretical depth and practical inside. Academic Director: Prof. Dr. Christian Boller
The following lecturers are not complete: Prof. Tadeusz Stepinski, Prof. Wieslaw Staszewski, Prof. Frank Walther, Prof. Giovanni Bruno, Prof. Gerd Dobmann, Prof. Philippe Guy
>

ISONIC 3510

Very Powerful Superior Performance Extremely Portable Smart Phased Array Ultrasonic Flaw Detector an
...
d Recorder with 2 Conventional UT and TOFD Channels uniquely combines PA, single- and multi-channel conventional UT, and TOFD modalities providing 100% raw data recording and imaging. Suitable for all kinds of every-day ultrasonic inspections
>

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window