06:19 Jul-29-2000
attenuation measurement for HIC

When measuring attenuation due to the suspected HIC,can anyone provide me acceptance and rejection criteria
based on the value of this attenuation? This is in order to assist our clients to do preventive measures
to theirs components.
Thank you.


 
 Reply 
 
Jairo Humberto Guzman
NDT Inspector, NDT researcher
Ecopetrol ICP, Colombia, Joined Nov 1998, 6

Jairo Humberto Guzman

NDT Inspector, NDT researcher
Ecopetrol ICP,
Colombia,
Joined Nov 1998
6
05:50 Jul-31-2000
Re: attenuation measurement for HIC
: When measuring attenuation due to the suspected HIC,can anyone provide me acceptance and rejection criteria
: based on the value of this attenuation? This is in order to assist our clients to do preventive measures
: to theirs components.
: Thank you.
Dr.Khazali Zin We have made some HIC inspecitions and we use 4Th eco to measurement the atenuation. we calibrate the 4Th eco to 80% of the screnn and the aceptance criteria is:
signals less than 20% of the screen have to be reyected.
Complementary you have to measuremet The backscater eco and velicities ratio.
The three methodes will give you the % of damage

good luck




 
 Reply 
 

Product Spotlight

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window