where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

1220 views
Technical Discussions
David Davies
Level III , QA Engineer , Ops. Supervisor
Vetco Saudi Arabia Ltd, Saudi Arabia, Joined Sep 2000, 3

David Davies

Level III , QA Engineer , Ops. Supervisor
Vetco Saudi Arabia Ltd,
Saudi Arabia,
Joined Sep 2000
3
01:02 Oct-12-2000
Automated UT of pipelines

I am evaluating a project for automated UT of cross country pipeline girth welds. Can anyone give me their experiences with the various options available, particularly capabilities, reliability, approval by certification bodies. I have a lot of experience with manual UT but need help with the latest automated equipment.
I am starting from scratch on this project so any pointers or contacts would be appreciated.
Thanks
Dave Davies


 
 Reply 
 
Doug Breeze
Director, Consultant; R&D
Inspection Software Limited, United Kingdom, Joined May 2000, 20

Doug Breeze

Director, Consultant; R&D
Inspection Software Limited,
United Kingdom,
Joined May 2000
20
01:22 Oct-13-2000
Re: Automated UT of pipelines
Trying to get on-the-record objective views from
users of automatad equipment must be like asking
a preacher which is the best God.

My comments are no more objective than anyone else's,
but they are based on field experience with several
automated systems (some nuclear, some pipelines,
some in the Saudi desert), but there are several
common principles to look for.

The Equipment
-------------
1. Look at the suppliers reputation and track record.
2. Look for the very best mechanical design...
(ruggedness, mechanical backlash, precision,
exposure/protection, connections, etc.)
3. Look for flexibility and versatilty in the software,
best performance in the electronics, and for a
range of scanners... whatever you plan to examine
now, you'll need to do something different soon
enough.
4. Plan for regular maintenance schedules (sometimes
daily in the desert), and determine how readily the
systems strip apart for cleaning and maintenance.


The Operators
-------------
1. Automated kit needs to be loved, by dedicated, well
qualifed operators. Don't be misled into planning
to use lesser grade personnel.
2. Aim to employ multi-discipline supervisors with
competence in UT, electronics, mechanics,
computers, etc., and with practical skills too.
3. Plan to have the operators fully trained in
operation AND maintenance, by the manufacturer.

Trust this helps.


 
 Reply 
 
John O'Brien
Consultant, -
Chevron ETC , USA, Joined Jan 2000, 281

John O'Brien

Consultant, -
Chevron ETC ,
USA,
Joined Jan 2000
281
01:50 Oct-18-2000
Re: Automated UT of pipelines
Most of the providers are following the zonal approach originally developed out of Canada (Ed Ginzel whose input you will often see on NDTNET) was a leading figure in this.

Some systems add in TOFD as an extra channel for detection but sizing is still mainly Pulse Echo with cross talking probes focussed on different weld zones.

RD tech, AIS/Weldsonix, RTD, Vincotte, SSI SGS Gottfeld all use similar approaches.

The technique is well accepted in many areas now Canada, Gulf Of Mexico, Gaz De France, Petrobras etc. etc.

University Of Ghent in Belgium has been running and assessment project including the application and comparison of Phased Array technology which is seen by some as the next direction.

Acceptance Criteria is the biggest issue people like NOVA have direct specs now but API 11.04 does not and you need to consider the FFS Appendix and an ECA for determining new accepatnce criteria.

If procuring equipment other issues come into play such as reliability.

We have assisted in development projects in this area so if you need direct input please contact me.




 
 Reply 
 
Tim Sun
Tim Sun
08:28 Oct-23-2000
Re: Automated UT of pipelines



 
 Reply 
 
Michael Moles
, Joined ,
01:13 Nov-03-2000
Re: Automated UT of pipelines
: I am evaluating a project for automated UT of cross country pipeline girth welds. Can anyone give me their experiences with the various options available, particularly capabilities, reliability, approval by certification bodies. I have a lot of experience with manual UT but need help with the latest automated equipment.
: I am starting from scratch on this project so any pointers or contacts would be appreciated.
: Thanks

R/D Tech manufactures a phased array system for inspecting girth welds, called PipeWIZARD. There are several references at conferences (e.g. ASNT) as well as electronic versions (see 15 WCNDT). Phased arrays have major advantages over conventional systems: smaller; lighter; can scan from 4" to 56"with same arrays; load a sset-up electronically; increased number of zones for better sizing etc. Check our web site.
: Dave Davies




 
 Reply 
 
Thomas S Connelly
Thomas S Connelly
09:44 Nov-28-2000
Re: Automated UT of pipelines
: I am evaluating a project for automated UT of cross country pipeline girth welds. Can anyone give me their experiences with the various options available, particularly capabilities, reliability, approval by certification bodies. I have a lot of experience with manual UT but need help with the latest automated equipment.
: I am starting from scratch on this project so any pointers or contacts would be appreciated.
: Thanks
: Dave Davies

One should be very careful when selecting the Company, in areas like experience, equipment, prosed sizing method, spares etc.

It would also be invaluable to send your proposed specifications to the companies and determine how they will meet the specification. A validation of the companies using defective welds would also help.

Determine the flaw sizing methods to be used i.e. Zonal, amplitude, combination and any other.

beware of how companies or individuals attempt to apply the appendix of API 1104. Monitor carefully how the company intend to apply workmanship standards.

Certain consultants or field experts may wish to overcomplicate AUT it does not have to be over elaborate but MUST be adequate for the required inspection project.

My employers offer a full consulting and quality service for mechanized UT including field and online (remote) audit, validations, qualification etc

Regards

T. S. Connelly




 
 Reply 
 
Steve Jones
, Joined ,

Steve Jones

,
Joined

06:10 Nov-29-2000
Re: Automated UT of pipelines



 
 Reply 
 

Product Spotlight

On Demand Webinar: Improve the Efficiency and Accuracy of Inspection Scanning

On-demand webinar on scanning technology that helps improve the efficiency and accuracy of ultrasoni
...
c inspections in oil and gas, aerospace, manufacturing and other industrial applications. The webinar features a scanning solution for multiple inspection environments, including flat and curved specimens, magnetic and nonmagnetic surfaces and raster scanning over long distances. View it today.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window