ashraf samir
03:55 Apr-27-2001
X Ray for 2" thickness pipeline

our next project is 2" thickness offshore pipeline , we need to applly ndt to the welds , shall X Ray be able to inspect the welds or we need another method , i have J.M.E crawler .



 
 Reply 
 
Guido Crapels
Guido Crapels
09:47 Apr-27-2001
Re: X Ray for 2" thickness pipeline
: our next project is 2" thickness offshore pipeline , we need to applly ndt to the welds , shall X Ray be able to inspect the welds or we need another method , i have J.M.E crawler .
.
Reply:

For this kind of thicknesses x-ray is not suitable. Conventional x-ray tubes cannot produce energies sufficiently high for useful radiographies of welding defects (theoretically, a linear accelerator could do the job, but will not fit onto a crawler and is way too large and expensive to be handled outside any dedicated facility). You would need something like a Co60 source, but this is not suitable regarding safety. The conventional Ir192 source (with lower energy) could theoretically meet the testing quality requirements (maybe), but would take a rather long exposure time and is therefore unlikely to be economical.
Even if you could qualify a radiography test in this case, the weld will comprise many layers in which small flaws can hide that will not be detected by radiography.
In most cases these kind of welds are examined by means of ultrasonics, like the RTD Rotoscan system. It is fast and produces the information required for proper testing for flaws like slag inclusions, lack of fusions and root flaws. The pulse-echo mode can be combined with Time of Flight testing in the same run. This technique is qualified for all major Pressure codes, on- and offshore likewise.



 
 Reply 
 
Doug Breeze
Director, Consultant; R&D
Inspection Software Limited, United Kingdom, Joined May 2000, 20

Doug Breeze

Director, Consultant; R&D
Inspection Software Limited,
United Kingdom,
Joined May 2000
20
09:40 Apr-27-2001
Re: X Ray for 2" thickness pipeline
: our next project is 2" thickness offshore pipeline , we need to applly ndt to the welds , shall X Ray be able to inspect the welds or we need another method , i have J.M.E crawler .
.
Wall thickness of 2" is very substantial. If this is
the real thickness then automated UT will be cheaper,
faster, more sensitive, and safer than any X-Ray
or Gamma-Ray crawler.

Take a look at http://www.inspection.co.uk or
http://www.force.dk for info on 'P_scan System 4'
and 'P-scan 4 Lite' systems.

Remember that you'll need fully trained and
experienced technicians to get the best out of any
automated UT system.


 
 Reply 
 
Massimo Carminati
Massimo Carminati
07:10 Apr-28-2001
Re: X Ray for 2" thickness pipeline
You can also check on the R/D Tech web site and look for more information on the Phased Array Pipe Wizard system. It is the most advanced system available fpr automated UT and the use of Phased Arrays may reduce the number of probes (in this case) by a factor of 10!


 
 Reply 
 
rajeev chaudhari
NDT Inspector
offshore testing & inspection services (I) pvt ltd, India, Joined Dec 2000, 17

rajeev chaudhari

NDT Inspector
offshore testing & inspection services (I) pvt ltd,
India,
Joined Dec 2000
17
02:20 Apr-28-2001
Re: X Ray for 2" thickness offshore pipeline
OTISLAB has complete facilities for NDT testing for various requirements. If you could let us know ID, OD, it will be easy to decide extact technique and equipment cababilities. We hope you will understand implication of incorrect details.





 
 Reply 
 
ender keskin
ender keskin
06:30 May-30-2001
x-ray apparatus for pipeline(up to 1" pipeline)
we are looking for x-ray apparatus for 14mm-16mm pipeline(meat thickness)
could you inform us where and which brand are we going to search?
could you give some e-mails,adresses,tels or any other connections?
we want to buy one asap.

best regards,

ender keskin


 
 Reply 
 
ender keskin
ender keskin
06:35 May-30-2001
pipeline
we are looking for grounding conducter,welder protctive tent,insulation detecting device,pipe bending machine and boring machine.
pls contact with us asap..

best regards,

ender keskin


 
 Reply 
 

Product Spotlight

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

NEW! The PragmaPro Instrument Platform

The PragmaPro is based on a modular cartridge technology and supports various NDT instrument modal
...
ities such as UT, PAUT, ECT and many more. This new platform is based on a machined, powder-coated aluminum frame for shock-proofness, best sealing qualities and maximum heat dissipation. This is practical to extend the outdoor temperature range and/or to extend the power injected in the transducers. The PragmaPro is aiming at a very wide range of applications, such as weld scanning, corrosion mapping and composite testing.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window