UT for disbonding

Hello,
we have the task to test for disbonding of SS 1.4550 using SAS4IG (nearly similar material) as weld metal. The thickness of weld metal is appr. 3 mm. Testing should be performed using SDH as reflectors. the test block has a diameter of 273 mm (not ready yet). The test object is ready next Monday.
I prepared a MSEB4, E series, to be adapted at the curvature of 273 mm.
But now I am not sure if it is the right probe. Should`nt I use higher frequencies?
For any hints or advices I thank You in advance
Joerg

 
 Reply 
 
Luis Ganhao
Engineering,
USA, Joined Sep 2008, 25

Luis Ganhao

Engineering,
USA,
Joined Sep 2008
25
16:51 Mar-19-2009
Re: UT for disbonding
In Reply to Joerg Neubert at 16:30 Mar-19-2009 (Opening).

The best probes for disbonding detection are the benchjmark and between 10-15 MHz because you you need haigh resolution for diferentiate the metal base and the SS interface

 
 Reply 
 
Theo Micottis
Theo Micottis
10:04 Jul-14-2009
Re: UT for disbonding
In Reply to Luis Ganhao at 16:51 Mar-19-2009 .

Hello,
I have to verify disbonding using ASME IV Technique two.The customer haven't gave me the standard of acceptance yet.Which could be an acceptance standard for ASME?
Thank you in advance
THEO

 
 Reply 
 

Product Spotlight

Echomac® PA Tube Weld Tester

The new robotic Echomac® PA TW is an operator friendly test system for detecting weld zone defects
...
in tube and pipe caused by scarfing or welding processes. Electronic scanning ensures that the entire weld zone is covered without the need for mechanical movement or operator adjustment.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

MANTIS

MANTIS is a compact, powerful and affordable flaw detector (16:64PR), dedicated to field operators
...
. This portable equipment offers standard (electronic-, sector-, compound scan, conventional UT for pulse-echo, dual array and TOFD inspections), and advanced phased-array (real-time TFM -Total Focusing Method). MANTIS benefits from the same intuitive and user-friendly interface (CAPTURE) than Gekko for easier inspections.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window