10:01 Jun-23-2009
stainless steel tofd inspection

hello all teachers:
stainless steel do tofd inspection ok or not? and workpiece material is TP321 which is pressure pipe, I do some experiments, two probes at weld one side, inspection HAZ and material , tofd image is good ,but two probes across weld(one is left of weld ,one is right),tofd image is not good , probe frequency is 1.6MHz and crystal size is 6mm, so I want to solve this problem,thanks

 
 Reply 
 
Honda_Jazz
Honda_Jazz
15:26 Jun-23-2009
Re: stainless steel tofd inspection
In Reply to rocklee at 10:01 Jun-23-2009 (Opening).

What i know la, TOFD cant do on SS material bcoz this material have coarse grain structure and TOFD very2 high sensitivity and effect to the TOFD image.How can we interpret that image if Blur n dark..

 
 Reply 
 
luis ganhao
Engineering,
USA, Joined Sep 2008, 25

luis ganhao

Engineering,
USA,
Joined Sep 2008
25
15:56 Jun-23-2009
Re: stainless steel tofd inspection
In Reply to rocklee at 10:01 Jun-23-2009 (Opening).

TOFD is one of the best techniques for weld inspection include SS now regards your email the frquency used is very low you have increment it of course this depends the thickness under examination and the size of your transduceres is Ok. Try with 5-10 MHz

 
 Reply 
 

Product Spotlight

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window