14:39 Oct-01-2009
B31.1 / B31.3 Piping UT with TOFD method

Hello,
One of our customer wants TOFD method for their B31.1 piping Heavy wall pipes. They also wants in use of TOFD technique in lieu of Conventional or PA UT methods.
can we use TOFD method in power or process piping according to code cases 179-181 ?
or is there any restriction to use TOFD under the B31.1 or 31.3 piping codes ?

 
 Reply 
 
Luis Ganhao
Engineering,
USA, Joined Sep 2008, 25

Luis Ganhao

Engineering,
USA,
Joined Sep 2008
25
16:30 Oct-01-2009
Re: B31.1 / B31.3 Piping UT with TOFD method
In Reply to ihsan Duzgun at 14:39 Oct-01-2009 (Opening).

the code case 181 permit the use of AUT (TOFD & PA) in lieu of RT, but you have to select the most appropriated setting for the examination, I mean you need to check the thickness and after that select de frequency, probe sizes and angles. Regards to the calibration block ASME Sec V Appendix III and BSI-7706 or ENV-583-6 given to you the chance to perform the calibration for TOFD on the pipe material to be inspected. But you need a calibration block for shear wave (this technique is necessary to check the dead zones of TOFD). I have carried out many inspections on pipelines with TOFD in lieu of RT, whose thicknesses were in the order of 9-70 mm, inclusive I could detect cracks generated by service (gas).

I hope this can help you

 
 Reply 
 
luis ganhao
Engineering,
USA, Joined Sep 2008, 25

luis ganhao

Engineering,
USA,
Joined Sep 2008
25
16:41 Oct-01-2009
Re: B31.1 / B31.3 Piping UT with TOFD method
In Reply to ihsan Duzgun at 14:39 Oct-01-2009 (Opening).

Sorry, but the appendix III from ASME SEC V does not apply fro piping (calibration block) so you need is the specifications for your block found in the code case 181, however the BSI-7706 give you the option for calibration over the pipe that you want inspect, I mean this std. offer 4 or 5 different forms to obtain the minimal sensitivity besides you can use the BSI-14751 or ENV-583-6

 
 Reply 
 
ihsan Duzgun
NDT Inspector, NDE Supervisor
Cimtas Piping Industries Ltd. Co., Turkey, Joined Sep 2009, 4

ihsan Duzgun

NDT Inspector, NDE Supervisor
Cimtas Piping Industries Ltd. Co.,
Turkey,
Joined Sep 2009
4
16:57 Oct-01-2009
Re: B31.1 / B31.3 Piping UT with TOFD method
In Reply to Luis Ganhao at 16:30 Oct-01-2009 .

under the light of code case allows TOFD for B31.3 applications but what about B31.1 power piping ? In code case 179 sect (d) it says about indication evaluation "20% of the reference level shall be investigated to extent UT exam" means DAC and i understand that only amplitude based UT methods shall be permitted and also B31.1 piping refers to ASME sect V article 4 if we check the equipment requirements under T-430/T-431 again we can see "a pulse echo type instrument shall be used" criteria. As far i know TOFD method (im not familar to TOFD applications) is not a pulse-echo or amplitude based UT technique ?
in my opinion, it isnt clear that using TOFD technique in lieu of conventional or PH UT methods for B31.1 Power piping ?

 
 Reply 
 

Product Spotlight

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

VeeScan AirCraft Wheel Inspection

The VEESCAN offers maximum flexibility, has a proven mechanical design and records of breakdown-fr
...
ee operation of over 365 days. Appealing to companies in the Aerospace industry, the VEESCAN is ideal for all wheel-testing environments. With a wide selection of probes, the VeeScan allows your wheel testing facility the flexibility to select the most compatible configurations with their workload.
>

Extended Range Variable Wall® Piping Calibration Blocks for Longseam Inspection

This set of two blocks has been specially designed for situations where ultrasonic examination tak
...
es place circumferentially or “around the curve” for applications such as inspection of longseam welds in piping and vessels. Jointly designed by PH Tool and Holloway NDT, the blocks feature side-drilled hole reflectors positioned within novel compound-curves, each with multiple thickness steps. The unique design results in a light and compact form factor, with the largest block weighing just over 15 lbs and spanning just 16 ¾”. Coverage is provided for nominal pipe sizes from 6” to 10” in the small block and 12” to a whopping 56” in the large block. The compound OD curves and multiple wall thicknesses actually exceed ASME requirements, providing exceptional signal response and measurement accuracy. Properly managing beam divergence off the ID and stabilizing beam skew due to probe rocking is essential to maintaining a consistent calibration when inspecting lengthwise on curved surfaces.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window