what's this film of rt looks like?



Pipeline 273*7mm

 
 Reply 
 
anjafo79
NDT Inspector
Norway, Joined Aug 2009, 204

anjafo79

NDT Inspector
Norway,
Joined Aug 2009
204
11:42 Jan-22-2010
Re: what's this film of rt looks like?
In Reply to ligang feng at 02:59 Jan-22-2010 (Opening).

looks like suck back on the root to me.

 
 Reply 
 
Phil
NDT Inspector, Radiation Safety
BINDT, MIAQP, United Kingdom, Joined Mar 2009, 151

Phil

NDT Inspector, Radiation Safety
BINDT, MIAQP,
United Kingdom,
Joined Mar 2009
151
17:31 Jan-22-2010
Re: what's this film of rt looks like?
In Reply to ligang feng at 02:59 Jan-22-2010 (Opening).

Looks the same to me as well

 
 Reply 
 
anjafo79
NDT Inspector
Norway, Joined Aug 2009, 204

anjafo79

NDT Inspector
Norway,
Joined Aug 2009
204
18:54 Jan-22-2010
Re: what's this film of rt looks like?
In Reply to Phil at 17:31 Jan-22-2010 .

looks acceptable to me as well with out cross checking wall thickness and accept criteria.

not darker than parent material either i guess

 
 Reply 
 
BILL KIESEL
BILL KIESEL
21:15 Jan-22-2010
Re: what's this film of rt looks like?
In Reply to ligang feng at 02:59 Jan-22-2010 (Opening).

looks like local negative reinforcement at the weld root, possable stress riser due to sharp appearance, definite failure point for this weld under extreme stress.

 
 Reply 
 
Phil
NDT Inspector, Radiation Safety
BINDT, MIAQP, United Kingdom, Joined Mar 2009, 151

Phil

NDT Inspector, Radiation Safety
BINDT, MIAQP,
United Kingdom,
Joined Mar 2009
151
23:04 Jan-22-2010
Re: what's this film of rt looks like?
In Reply to ligang feng at 02:59 Jan-22-2010 (Opening).

What is this pipeline for, what is flowing through it ?

Also which specification are you working to ?

As this will determine whether or not it is acceptable, as we know the size and wt.

 
 Reply 
 
Collin Maloney
NDT Inspector, - Plant Inspector
Applus RTD, Australia, Joined Nov 2000, 147

Collin Maloney

NDT Inspector, - Plant Inspector
Applus RTD,
Australia,
Joined Nov 2000
147
05:21 Jan-23-2010
Re: what's this film of rt looks like?
In Reply to ligang feng at 02:59 Jan-22-2010 (Opening).

look suspiciously like a burn through given that the profile of the root bead changes from thin to wide either side of the discontinuity.
I would like to know the welding technique used i.e. stove pipe. The cap weave looks typical of a stove technique. What was the o'clock position?

 
 Reply 
 

Product Spotlight

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window