Ketos Ring

dear all!
how do you make the ketos ring? i have Draw( refe to E1444), good mechanic but i have not any information material ? is it low carbon material?
Regard

 
 Reply 
 
Rolf
Director,
NDT.net, Germany, Joined Nov 1998, 617

Rolf

Director,
NDT.net,
Germany,
Joined Nov 1998
617
19:06 Feb-25-2010
Re: Ketos Ring
In Reply to Trinh Duy Dong at 18:54 Feb-25-2010 (Opening).

I edited your spelling from 'kentos ring' to 'keto ring'. If you search the forum or web for ketos ring you will find better information.

 
 Reply 
 
rafid O. Lopez
rafid O. Lopez
22:58 Feb-25-2010
Re: Ketos Ring
In Reply to Rolf at 19:06 Feb-25-2010 .

Is more easy that you buy the Ring AS5282, is the same that Ketos Ring but wih more sensibility the diference is the annealing. Is difficult to find the ketos ring, and to make it more; many vendors say they sell the ketos ring, but really is the as5282 ring.

Best regards.

 
 Reply 
 
Jim Draper
Consultant, ASNT Level III MT PT RT VT
Draper NDT, USA, Joined Jul 2009, 99

Jim Draper

Consultant, ASNT Level III MT PT RT VT
Draper NDT,
USA,
Joined Jul 2009
99
16:53 Feb-27-2010
Re: Ketos Ring
In Reply to rafid O. Lopez at 22:58 Feb-25-2010 .

The material is AISI 01 tool steel from annealed round stock, hardness 90 to 95 HRB.

 
 Reply 
 

Product Spotlight

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Research and Application Development For NDT

Acuren’s Research and Application Development specializes in the development of advanced ultraso
...
nic inspection techniques and systems for challenging inspection applications, with an emphasis on practical solutions which are field deployable. Services include manual and automated ultrasonic inspection system development, inspection technique optimization using laboratory scale studies and ultrasonic modeling (CIVA, BeamTool), preparing technical justification for technique evaluation and qualification (Probability of Detection and sizing accuracy studies), inspection/calibration/analysis procedure preparation to support field deployment of custom techniques, and development of custom imaging algorithms to support challenging inspection applications.
>

Extended Range Variable Wall® Piping Calibration Blocks for Longseam Inspection

This set of two blocks has been specially designed for situations where ultrasonic examination tak
...
es place circumferentially or “around the curve” for applications such as inspection of longseam welds in piping and vessels. Jointly designed by PH Tool and Holloway NDT, the blocks feature side-drilled hole reflectors positioned within novel compound-curves, each with multiple thickness steps. The unique design results in a light and compact form factor, with the largest block weighing just over 15 lbs and spanning just 16 ¾”. Coverage is provided for nominal pipe sizes from 6” to 10” in the small block and 12” to a whopping 56” in the large block. The compound OD curves and multiple wall thicknesses actually exceed ASME requirements, providing exceptional signal response and measurement accuracy. Properly managing beam divergence off the ID and stabilizing beam skew due to probe rocking is essential to maintaining a consistent calibration when inspecting lengthwise on curved surfaces.
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window