where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

Materials Research Institute
Consulting to the NDT industry.
4743 views
Articles & News
wolfgang Bisle
R & D, senior Engineer and nomiated Expert
retired from Airbus Deutschland GmbH, Germany, Joined Jul 2000, 35

wolfgang Bisle

R & D, senior Engineer and nomiated Expert
retired from Airbus Deutschland GmbH,
Germany,
Joined Jul 2000
35
19:02 Jan-06-2011
Characterization of the effects of Water and Disbond on Ultrasonic Signals in Honeycomb Composite Structures
Overall
Style
Insight
Reliability

This article shows a typical student sight of that theme with limited practical background. I think the student is not responsible about the quality of the approach but the tutor should have better insight to guide a young fellow.
The solution proposed is not state of the art. I recently did a presentation on the ATA NDT Forum covering a very similar subject - NDT Toolbox for Honeycomb Sandwich Structures/
http://www.airlines.org/SafetyOps/EM/Documents/2010%20NDT%2018%20Toolbox%20for%20Honeycobm%20Sandwich%20Structures.pdf
The use of neutron radiography is for me a totally overpowered method, the same can be rached by thermography (long pulse, flash, modulation) - see my presentation, we showed several very successfull options - as well with radiography. A well trained inspector quickly can interprete singal from both method, especially Thermography is a cheap and highly portable solution, where you must not disassemble control surfaces from the aircraft. This is especially valid in case of vertical structures like rudders.
Another approach is single side applied Ultrasonic - using low frequencies (250-800KHz), for detecting disbonds this method is limited to nearly parallel-skin honeycomb structures as it uses a guided wave approach resonating with the cell walls. For detecting fluid ingress it works also on tapered structures - see the mentioned presentation. We lack currently powerfull UT array transducers in the range of 0.5..1 MHz, now only one Imasonic transducer nearly fits our needs (but others are catching up); In case the mentioned Guided Wave approach is finally completely transferred to Array Transducers, there will be an extremly fast inspection method available, even coupling problems on aged and contaminated surfaces can be overcome wtih a new revolutionary way of coupling - we are working on this.
But neutron radiography and squirter UT is not necessary and inspecting wet is overcome by aircoupled UT or as others say "NCU" see
http://www.dr-hillger.de/Inhalte/Englisch/Luftultraschall_e.html

 
 Reply 
 
Thomas Krause
Thomas Krause
19:12 Jan-07-2011
Re: Characterization of the effects of Water and Disbond on Ultrasonic Signals in Honeycomb Composite Structures
In Reply to wolfgang Bisle at 19:02 Jan-06-2011 (Opening).

Wolfgang, I agree that water ingress is detectable by various forms of ultrasonics and thermography. However, to my knowledge only through-transmission ultrasonics has the potential to determine whether or not disbond is present when water is also present in the adjoining honeycomb cells. This was the point of the presentation.

 
 Reply 
 
Wolfgang Bisle
R & D, senior Engineer and nomiated Expert
retired from Airbus Deutschland GmbH, Germany, Joined Jul 2000, 35

Wolfgang Bisle

R & D, senior Engineer and nomiated Expert
retired from Airbus Deutschland GmbH,
Germany,
Joined Jul 2000
35
15:48 Jan-10-2011
Re: Characterization of the effects of Water and Disbond on Ultrasonic Signals in Honeycomb Composite Structures
In Reply to Thomas Krause at 19:12 Jan-07-2011 .

Download ATA NDT Forum 2007 Hicken - Rudders structural inspectionsPresented

Dear Thomas,
Sorry but I guess you are not following the technology applied to aircraft, especially not to Airbus aircraft.
Since a lot of years there are procedures included in the NonDestructive Tesing Manuals of all Airbus families, using the approach I described in my posting. It has also been presented in several ATA NDT Fori (or shall I say Forums) by my colleagues and so it can be said it is industry standard. Even if you go back to the homepage of Olympus you will find the method described there as UT bond testing for rear side debonding of sandwiches.
If you go for
http://www.olympus-ims.com/en/ndt-application/183-id.209715294.html
and head down to the paragraph "Conventional Ultrasonic Testing" the principle of the method is described there.
Dr. Hillger offers a special system for those inspections, if you look to the last page of this flyer
http://www.dr-hillger.de/PDF/LF_Ultrasonics.pdf
you will see a picture using this technique an Al honeycomb structures.
Refer also to this article:
http://www.ndt.net/article/ecndt98/aero/011/011.htm
and the DAMDOS Project.
Some of the older presentation of e.g. ATA NDT Forum 2007 are not available on the net anymore.

So as you see, sometime industry is maybe far ahead of research - call e.g. the colleagues of Air Canada, they should have used this method already....
Or ask the colleagues of Olympus in Quebec, we have discussed this method already years ago with them, you see the result is the application note in their Homepage.

Summing up: Detecting water with single sided UT in Honecomb is simple methods, which is industry standard. (If you focus on the capability to differentiate between indication showing only a disbond or showing only the presence of water:
With the method I presented here, you can do this differentiation only of the cells are horizontal so that water has contact with the surface where you place the transducer. If you place the transducer on a horizontal placed sandwich where the cells are situated vertical, disbond and water ingress may produce the same indication (in theory the water completely damps the signal, a disbond reduces between 6 and 12 dB., But in reality such structures have lot of variations that this differentiation cannot be made. So the threshold in our procedures is always signal reduction of more than 6 dB, after adjustment on the structure (not on a separate reference block) as production of sandwich has a big variance and reference blocks never (!!!) show the same behavior like real in service structure. We have tested this method now between high arctic and tropical rain forest - from dessert to seaside, on new but also on aged structures - a POD is existing - look for the ATA NDT Forum presentation I have referenced

http://www.airlines.org/SafetyOps/EM/Documents/2010%20NDT%2018%20Toolbox%20for%20Honeycobm%20Sandwich%20Structures.pdf

This presentation may give you especially on Foil 13..16 the necessary information
I uploaded also the 2007 presentation.
 
 Reply 
 
Norm Woodward
Norm Woodward
18:04 Jan-26-2011
Re: Characterization of the effects of Water and Disbond on Ultrasonic Signals in Honeycomb Composite Structures
In Reply to wolfgang Bisle at 19:02 Jan-06-2011 (Opening).

Wolfgang-

I agree that neutron radiography (N-ray) should be considered "overpowering," but this is generally the opinion of nearly everyone who doesn't own one, and can’t afford one. As the student said, he was hoping to offer a solution to the current problem, that the scheduled detection of disbonds by TTU was being baffled in the presence of water. The use of N-wave was only to graphically demonstrate that he was able to separate disbonds from water, and he was not suggesting N-ray to routinely detect either.

BTW, one of the few advantages of N-ray is that it is not hindered by such nuisances as unaligned (metallic) honeycomb cells and the presence of fasteners, thereby eliminating the problems you seemed to have with x-ray. [It does, however, share the problem of separating water from globs of organic sealants/adhesives.]

I am glad you are enthralled with thermography, though your advocacy of such enhancements such as baking and freezing introduces of such unintentional consequences as core blowouts due to sudden water evaporation, or core ruptures due to water freezing and expanding.

With all due respect to your commercial aviation background, from the military prospective of doing the best with what you have on hand, I thought the student handled his mission admirably.

Respectfully yours,
Norm

 
 Reply 
 

Product Spotlight

Ultrasonic Probe Recharacterization Service

NDT Systems offers a comprehensive Aftercare and Recharacterization Service for all our ultrasonic
...
probes. The Recharacterization Service is fully compliant with International ASTM E1065 Standard Guide (and other applicable standards) and offers complete documentation, traceable to the ASTM E1065 Standard. For more details or to schedule Recharacterization Services contact ndtsales@ndtsystems.com
>

VeeScan AirCraft Wheel Inspection

The VEESCAN offers maximum flexibility, has a proven mechanical design and records of breakdown-fr
...
ee operation of over 365 days. Appealing to companies in the Aerospace industry, the VEESCAN is ideal for all wheel-testing environments. With a wide selection of probes, the VeeScan allows your wheel testing facility the flexibility to select the most compatible configurations with their workload.
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window