06:59 Dec-11-2001
NDE of Thermal Spray Coatings


I would like to know if anybody has experience in NDE of Thermal Spray Coatings. I am looking for mainly:
- Adhesive Bond Strenght Determination by Ultrasonics and/or other related NDE methods
- Integrity of Thermal Spray Coatings: Determination of oxides, porosity, delaminations...

Thanks,
Nihat
General Electric Marmara Research Center


 
 Reply 
 
Jonathan Buttram
Engineering
USA, Joined Nov 1999, 1

Jonathan Buttram

Engineering
USA,
Joined Nov 1999
1
07:14 Dec-11-2001
Re: NDE of Thermal Spray Coatings
:We have applied EMAT technology toward the a couple of thermal spray applications. The first is related to bond coating integrity and thickness measurement, and the second is the development of a real-time monitoring sensor used in the application of the medium. All of these applications utilize ultrasonic methods without the need for couplant. Please feel free to contact me at Innerspec Technologies if more information is required. Thanks,
Jonathan Buttram (jdbuttram@innerspec.com)

: I would like to know if anybody has experience in NDE of Thermal Spray Coatings. I am looking for mainly:
: - Adhesive Bond Strenght Determination by Ultrasonics and/or other related NDE methods
: - Integrity of Thermal Spray Coatings: Determination of oxides, porosity, delaminations...
.
: Thanks,
: Nihat
: General Electric Marmara Research Center
.



 
 Reply 
 
Xavier
Xavier
02:19 Dec-12-2001
Re: NDE of Thermal Spray Coatings
I worked on a 2 years project related to the detection of delamination in thermal spray coatings metals (ceramic on top of a superalloy base metal). I investigated the use of ultrasonic testing (mainly using Lamb waves) but also infrared thermography.

In some cases we were able to obtain interesting results, but these depended greatly on the surface finish of the ceramic coating.

Also, for most application it is not very suitable to use ultrasonic testing since a couplant (either water or gel) can actually infiltrate the ceramic and may remain within the material. So we were trying to develop a non-contact and couplant-free inspection technique.

Unfortunately, we (the only 2 researchers involved in this project) have left the research institute where the research was carried out and we haven't been replaced. So I don't know if the project is still running.

Neverthless, it is very challenging but interesting task.

Good luck !

:
: I would like to know if anybody has experience in NDE of Thermal Spray Coatings. I am looking for mainly:
: - Adhesive Bond Strenght Determination by Ultrasonics and/or other related NDE methods
: - Integrity of Thermal Spray Coatings: Determination of oxides, porosity, delaminations...
.
: Thanks,
: Nihat
: General Electric Marmara Research Center
.



 
 Reply 
 

Product Spotlight

GEKKO, Standard and Advanced phased-array for Easier inspection

M2M Gekko® is a field-proven flaw detector offering PAUT, UT, TOFD and TFM through the streamline
...
d user interface Capture™. Released in 32:128, 64:64 or 64:128 channel configurations, Gekko combines high- resolution and speed while reducing inspectors’ training time.
>

Ultrasonic Testing Immersion Tanks with Unmatched Scanning Features

TecScan’s non-destructive testing Ultrasonic Immersion Tanks & scanners are designed for high pe
...
rformance and demanding NDT testing applications. Our Scan3D™ line of High Precision Immersion Tanks are specifically designed for automated ultrasonic testing of complex composites parts used in aerospace and industrial applications.
>

Robotic laser shearography enables 100% inspection of complex, flight-critical composite structures

An article in “Composites World Magazine” showcases Non Destructive Testing of aero-structures
...
with Laser Shearography. Over the years Dantec Dynamics has supplied many solutions for the aerospace industry. Referring to specific customer projects several of these cases are examined to outline the advantages of using Laser Shearography for automated defect detection.
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window