where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

WesDyne International (AMDATA Products)
WesDyne is an engineering and technical services firm dedicated to providing standard and custom nondestructive examinations (NDE) products and systems
3405 views
Technical Discussions
Klimaszewski
Engineering
Instytut Techniczny Wojsk Lotniczych, Poland, Joined Mar 2001, 2

Klimaszewski

Engineering
Instytut Techniczny Wojsk Lotniczych,
Poland,
Joined Mar 2001
2
04:10 Feb-21-2002
method for detection water in honeycomb

I am looking for a method/equipment (except X-ray) for detection water in aircraft structure consists of: al alloy skin + al alloy honeycomb).
Thank you in advance for any help.
S³awomir


 
 Reply 
 
Richard Fitch
Richard Fitch
05:04 Feb-21-2002
Re: method for detection water in honeycomb
: I am looking for a method/equipment (except X-ray) for detection water in aircraft structure consists of: al alloy skin + al alloy honeycomb).
: Thank you in advance for any help.
: S³awomir
.
We are developing a method using infra-red thermal imaging with good results so far. Please contact me if you require more information.


 
 Reply 
 
John Rodgers
John Rodgers
05:26 Feb-21-2002
Re: method for detection water in honeycomb
: I am looking for a method/equipment (except X-ray) for detection water in aircraft structure consists of: al alloy skin + al alloy honeycomb).
: Thank you in advance for any help.
: S³awomir
.
We previously developed a method using acoustic emission for the USAF that was very effective and used in maintenance for a number of years. It could find very small amounts of moisture (non-standing) by detecting corrosion activity. The process used a hot air gun to heat they local structure briefly, then monitoring with a single channel AE instrument for ~1 minute. This was done on 6-inch centers. It was used on Al honeycomb structure. This procedure could also be practiced in the field without removing structure. It was used to find and map very small amounts of corrosion, even where there was only a slight "frosting" of the honeycomb Al cells.


 
 Reply 
 
Chris Coughlin
Chris Coughlin
05:30 Feb-21-2002
Re: method for detection water in honeycomb
: I am looking for a method/equipment (except X-ray) for detection water in aircraft structure consists of: al alloy skin + al alloy honeycomb).
: Thank you in advance for any help.
: S³awomir
.

Microwave NDT has been used with tremendous success for this exact application as a relatively straightforward inspection. The Canadian military used to do a lot of work in this field, I don't know if they're still involved with it or not. A good starting point would be Dr. Zoughi's Applied Microwave Nondestructive Testing Laboratory at http://www.ece.umr.edu/amntl/.



 
 Reply 
 
Fernando Santos
Engineering
NDT EXPERT, France, Joined Jun 2000, 3

Fernando Santos

Engineering
NDT EXPERT,
France,
Joined Jun 2000
3
09:30 Feb-21-2002
Re: method for detection water in honeycomb
: I am looking for a method/equipment (except X-ray) for detection water in aircraft structure consists of: al alloy skin + al alloy honeycomb).
: Thank you in advance for any help.
: S³awomir
.
Shearography is a laser interferometry method able to detect water in al alloy skin + al alloy honeycomb. This method is certified for the inspection of the Concorde elevons and is now included in the Concorde NTM (Nondestructive Testing Manual). Concorde elevons are al alloy skin + al alloy honeycomb with skin thikcness ranging from 0.6mm to 3.5mm.
NDT Expert uses this method to inspect Air France Concorde fleet. If you have any further questions please don't hesitate to contact me.


 
 Reply 
 
Azarov N.T.
Engineering
GosNIIGA, Russia, Joined Jan 2000, 12

Azarov N.T.

Engineering
GosNIIGA,
Russia,
Joined Jan 2000
12
00:52 Feb-21-2002
Re: method for detection water in honeycomb
: I am looking for a method/equipment (except X-ray) for detection water in aircraft structure consists of: al alloy skin + al alloy honeycomb).
: Thank you in advance for any help.
: S³awomir


From Azarov N.T. (E-mail: azar@orc.ru,
ndt137@ncplg.msk.ru) the developer of ultrasonic instruments and process engineerings of a control, at your interest, is off-the shelf to consider problems of a control of water in honeycomb constructions used in aircraft construction .
Besides in Russian Civil aircraft this problem is solved completely: after detection of water the effective deleting and repair on the developed original process engineering will be carried out it. The characteristics of a ultrasonic method of a control of water in honeycomb constructions and it matching with a X-ray method are reduced below.

MATCHING
Characteristics of ultrasonic and X-ray methods control
of a content of water in bonded honeycomb constructions

¹ Parameter of control.
Ultrasonic method (UT).
X-ray method (RT).

1.Requirement to conditions of realization of a control:
UT. The control of honeycomb aggregates on a airplane at any time, including in winter conditions (is possible at a heating of an aggregate from an air field heat source), at a horizontal position of an aggregate or at declination up to 30 deg. The method of a control immersion, with local bath.
RT. Is possible) a control only of honeycomb aggregates removed with a airplane, in conditions of a hangar, in night .

2.Sensitivity:
UT - minimum a level of water in honeycomb, measuring of method 0,8mm.
RT - 2-3mm.

3.Productivity:
sq.m in hour. UT - 5-10 sq.m in hour.
RT - 1-2 sq.m in hour.

4. Possibility of measurement of a height of a pole of fluid in honeycombs and the definitions it of total volume in aggregate:
UT - are measured, representation of the information as C-scan, a mark of sites with water on a surface aggregate for consequent it extract.
RT - are not measured.

5.Complexity of a control on airplane of a type IL-86: UT - 510 norm. hour.
RT - 1500 norm. hour.

6. Radiation danger:
UT - is safe.
RT - is dangerous.

7. Power consumption and a mass of an equipment:
UT - 50 W, 15kg.
RT - 1500 W,150 kg.
N.T. Azarov




 
 Reply 
 
Norm Woodward
Norm Woodward
02:36 Mar-19-2002
Re: method for detection water in honeycomb
: I am looking for a method/equipment (except X-ray) for detection water in aircraft structure consists of: al alloy skin + al alloy honeycomb).
: Thank you in advance for any help.
: S³awomir
.

I wish you luck...

Despite some other claims at this thread, the USAF has not been especially satisfied with alternative methods of water detection, which has included thermography, neutron radiography, ultrasound, and, I guess, AE.

But there is good news. The two basic problems of radiography, safety and expense, can be significantly reduced.

We are currently using phosphor plate systems, as marketed by the major film manufacturers, to replace film, and 150kvp & 300kvp Golden pulsed x-ray sources to replace continuous potential sources.

Since the plates are reusuable, and the pulsed sources are nearly harmless beyond 20 ft (6 m), the economics and environmental improvements may cause you to rethink the abandoning of x-radiography.


 
 Reply 
 

Product Spotlight

Lyft™: Pulsed Eddy Current Reinvented

PEC Reinvented—CUI Programs Redefined Corrosion under insulation (CUI) is possibly the greatest u
...
nresolved asset integrity problem in the industry. Current methods for measuring wall thickness with liftoff, without removing insulation, all have severe limitations. Eddyfi introduces Lyft — a reinvented, high-performance pulsed eddy current (PEC) solution. The patent- pending system features a state-of-the-art portable instrument, real- time C-scan imaging, fast data acquisition with grid-mapping and dynamic scanning modes, and flexibility with long cables. It can also scan through thick metal and insulation, as well as aluminum, stainless steel, and galvanized steel weather jackets. Who else but Eddyfi to reinvent an eddy current technique and redefine CUI programs. Got Lyft?
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window