02:22 Nov-23-2011
material indentification

hello guys
I am trying to obtain an instrument that gives the carbon content of a given material. I know of Belec. Can any of you provide more information on manufacturers on first hand experience with these instruments.

    
 
 Reply 
 
LK
NDT Inspector,
Norway, Joined May 2008, 104

LK

NDT Inspector,
Norway,
Joined May 2008
104
16:15 Nov-23-2011
Re: material indentification
In Reply to eron at 02:22 Nov-23-2011 (Opening).

Google for ARCMET

    
 
 Reply 
 
franco benvenuto
NDT Inspector
Italy, Joined Sep 2009, 13

franco benvenuto

NDT Inspector
Italy,
Joined Sep 2009
13
21:41 Nov-24-2011
Re: material indentification
In Reply to eron at 02:22 Nov-23-2011 (Opening).

We use Spectro (we have more instruments and one is with carbon). It's easy to use.

    
 
 Reply 
 
Phil
NDT Inspector, Radiation Safety
BINDT, MIAQP, United Kingdom, Joined Mar 2009, 151

Phil

NDT Inspector, Radiation Safety
BINDT, MIAQP,
United Kingdom,
Joined Mar 2009
151
12:45 Nov-25-2011
Re: material indentification
In Reply to eron at 02:22 Nov-23-2011 (Opening).

Hi Eron

Yes the Company I work for also use Spectro we have 3 machines and all of them detect Carbon as well as other Elements you will not find with XRF.

Regards

    
 
 Reply 
 
eron
Worldwide, Joined Nov 2011, 5

eron

Worldwide,
Joined Nov 2011
5
01:23 Nov-29-2011
Re: material indentification
In Reply to Phil at 12:45 Nov-25-2011 .

thanks guys.
Does the spectro instrument also gives a grade match for different alloys?
Have anyone used the instrument from Belec?

    
 
 Reply 
 
Hari Kishore Maddi
NDT Inspector,
Sievert Group of Companies, India, Joined Nov 2011, 14

Hari Kishore Maddi

NDT Inspector,
Sievert Group of Companies,
India,
Joined Nov 2011
14
03:30 Nov-29-2011
Re: material indentification
In Reply to eron at 02:22 Nov-23-2011 (Opening).

Dear Eron, Mobile OES Spectrometer from M/s. SPECTRO is suitable for Assessing the carbon content in a material.

    
 
 Reply 
 
Phil
NDT Inspector, Radiation Safety
BINDT, MIAQP, United Kingdom, Joined Mar 2009, 151

Phil

NDT Inspector, Radiation Safety
BINDT, MIAQP,
United Kingdom,
Joined Mar 2009
151
15:55 Nov-29-2011
Re: material indentification
In Reply to eron at 01:23 Nov-29-2011 .

Hi Eron

The Spectro can not give a grade match for different alloys unless you have the material certificate to compare it with, also you have the program for the grade you are looking for to allow any thing you can call grade match.

Regards

    
 
 Reply 
 

Product Spotlight

Ultrasonic tomograph for imaging of concrete structures А1040 MIRA

Applicable for concrete inspection allowing imaging of the internal structure of objects from conc
...
rete, reinforced concrete, different stones. The operation applies pulse-echo technique at one-side access to the object. The instrument is feasible for concrete inspection for searching conduct ducts, conduits, detection of foreign inclusions, holes, honeycombing, cracks and other concrete defects.
>

Echomac® Small

Available with up to eight channels of electronics to detect and evaluate thickness, flaws and eccen
...
tricity, this UT tester is housed in a convenient, smaller cabinet. This instrument can be used in conjunction with bubbler or immersion tank systems, or with a test bench or in laboratory applications. The Echomac® Small is available in the FD4, FD6 or FD6A versions.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>

PROlineTOP Plug & Play Ultrasonic inspection device

As Plug & Play solution it units all control and operation elements in a small housing and therefo
...
re replaces the typical control cabinet...
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window