Inconel 825 Acoustic longitudinal velocity

I am trying to find the acoustic longitudinal velocity for Inconel 825. there is not much information posted about this alloy. Does any one have any ideas what the velocity is or where I might find it?


 
 Reply 
 
Danny Wang
Danny Wang
09:53 Jun-06-2002
Re: Inconel 825 Acoustic longitudinal velocity
: I am trying to find the acoustic longitudinal velocity for Inconel 825. there is not much information posted about this alloy. Does any one have any ideas what the velocity is or where I might find it?
.

John:

Velocity V=D/t Two techniques:
(1)
Find a place with known thickness (t) such as flange.
Using your UT to find the transient time ( delta T). The time from initial pauls to first back wall or the transient time from 1st back wall to 2nd back wall.

V= 2 x thickness/ delta T

(2)
Find a place with known thickness (t) such as flange.
Using your UT, placed a probe on the known thickness area and change the velocity until the first back to the correct thickness.

If you have futher question you can call me at 909-392-5263. or visit my web site at http://www.spectruminspection.org

Danny Wang, PE




 
 Reply 
 
Richard Finlayson
Director, Operations
Princeton Instruments, USA, Joined Jun 2000, 8

Richard Finlayson

Director, Operations
Princeton Instruments,
USA,
Joined Jun 2000
8
00:52 Jun-06-2002
Re: Inconel 825 Acoustic longitudinal velocity
: : I am trying to find the acoustic longitudinal velocity for Inconel 825. there is not much information posted about this alloy. Does any one have any ideas what the velocity is or where I might find it?
: .
.
: John:
.
John,

You can find a table of acoustic velocities in Part 2 of the NDT Handbook,UT testing,Volume Seven from ASNT. It shows the longitudinal wave velocity as 5820 m/s for Inconel.

Richard
Major (retired) Richard D. Finlayson
Director, Research, Engineering Applications, Certification,
Training (REACT) and New Business Development
Physical Acoustics Corp.
195 Clarksville Road
Princeton Jct. NJ 08550, USA
Direct Phone: (609)-716-4026
Fax: (609)-716-0706
e-mail: rfinlayson@pacndt.com
web site: www.pacndt.com




 
 Reply 
 
M. W. Moyer
M. W. Moyer
01:41 Jun-06-2002
Re: Inconel 825 Acoustic longitudinal velocity
I have the following values for Inconel:
Inconel 600 Inconel
Longitudinal Velocity: 5.915 mm/us 5.820 mm/us
Shear Velocity: 3.078 mm/us 3.020 mm/us
Density: 8.45 gm/cm^3 8.250 gm/cm^3

: I am trying to find the acoustic longitudinal velocity for Inconel 825. there is not much information posted about this alloy. Does any one have any ideas what the velocity is or where I might find it?
.



 
 Reply 
 

Product Spotlight

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

Compact NDT inspection-heads for measurements with active thermography

The compact inspection head is suitable for thermographic ndt tasks. The uncooled infrared camera
...
is specially developed for NDI-tasks and offers a thermal sensitivity until now known only from thermal imagers with cooled detector. All required components and functions are integrated into the inspection-head. You will only need an ethernet cable to connect the sensor with the evaluation system.
>

IntraPhase Athena Phased Array System

The Athena Phased Array system, manufactured by WesDyne NDE Products & Technology, consists of a pha
...
sed array acquisition system and PC running IntraSpect software. A PC is used to perform acquisition, analysis and storage of the data. System hardware is capable of operating up to four data sets with any combination of phased array or conventional UT probes. NOW AVAILABLE IN 64-64 CONFIGURATION.
>