Phased Array Detection Capability

Gents

Have someone experience at weld inspection, with main target on detection any corrosion, grooving on the ID, HAZ and base material up to 1 inch on pipe lines with combination of sectorial and angled linear groups. I need to inspect pipelines 23 mm thick. I have a probe 5L64 A12, Olympus made, What are the detection capability, etc.

Thanks, Regards

 
 Reply 
 
MAL HILL
United Kingdom, Joined Jun 2012, 14

MAL HILL

United Kingdom,
Joined Jun 2012
14
11:44 Aug-20-2013
Re: Phased Array Detection Capability
In Reply to Dalibor Aleksoski at 03:25 Aug-20-2013 (Opening).

TOFD is great for internal corrosion- as long as the external surfaces adjacent to the weld\HAZ are are smooth.Ive detected \resolved 1\2mm isolated corrosion on 12mm pipe -large areas of attack to the root are no problem-With snub nosed 15mhz specialist Phoenix probes 7mm pipes (focus on back wall) are even possible-Proved out with a suitable test piece

 
 Reply 
 
Dalibor Aleksoski
Macedonia, Joined Aug 2013, 7

Dalibor Aleksoski

Macedonia,
Joined Aug 2013
7
23:52 Aug-20-2013
Re: Phased Array Detection Capability
In Reply to MAL HILL at 11:44 Aug-20-2013 .

Thanks for the informations. I also prefer TOFD for corrosion/erosion detection. Only in my case I am very limited to use it, as a have to inspect elbows and I am limited to on side inspection only.
Regards

 
 Reply 
 
MAL
United Kingdom, Joined Jun 2012, 14

MAL

United Kingdom,
Joined Jun 2012
14
10:04 Aug-21-2013
Re: Phased Array Detection Capability
In Reply to Dalibor Aleksoski at 23:52 Aug-20-2013 .

Some companies orientate the TOFD probes parallel with the direction of travel (90 degrees turned to normal orientation) and tell the software that this is the orientation
Then you can scan large bends in bands along the bend-No good for small bore pipes though!!

 
 Reply 
 

Product Spotlight

Echomac® Small

Available with up to eight channels of electronics to detect and evaluate thickness, flaws and eccen
...
tricity, this UT tester is housed in a convenient, smaller cabinet. This instrument can be used in conjunction with bubbler or immersion tank systems, or with a test bench or in laboratory applications. The Echomac® Small is available in the FD4, FD6 or FD6A versions.
>

Lyft™: Pulsed Eddy Current Reinvented

PEC Reinvented—CUI Programs Redefined Corrosion under insulation (CUI) is possibly the greatest u
...
nresolved asset integrity problem in the industry. Current methods for measuring wall thickness with liftoff, without removing insulation, all have severe limitations. Eddyfi introduces Lyft — a reinvented, high-performance pulsed eddy current (PEC) solution. The patent- pending system features a state-of-the-art portable instrument, real- time C-scan imaging, fast data acquisition with grid-mapping and dynamic scanning modes, and flexibility with long cables. It can also scan through thick metal and insulation, as well as aluminum, stainless steel, and galvanized steel weather jackets. Who else but Eddyfi to reinvent an eddy current technique and redefine CUI programs. Got Lyft?
>

NEW! The PragmaPro Instrument Platform

The PragmaPro is based on a modular cartridge technology and supports various NDT instrument modal
...
ities such as UT, PAUT, ECT and many more. This new platform is based on a machined, powder-coated aluminum frame for shock-proofness, best sealing qualities and maximum heat dissipation. This is practical to extend the outdoor temperature range and/or to extend the power injected in the transducers. The PragmaPro is aiming at a very wide range of applications, such as weld scanning, corrosion mapping and composite testing.
>

Wireless TOFD scanner

Quick, accurate and highly reproducible welds testing. The System operates wirelessly and is compat
...
ible with any type of Windows based Laptop, Desktop or Tablet.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window