AM Anang
NDT Inspector,
-, Indonesia, Joined Oct 2001, 4

AM Anang

NDT Inspector,
-,
Indonesia,
Joined Oct 2001
4
17:06 Dec-02-2013
API 620 & ASME VIII Div.1

Dear All,

Application of ultrasonic test method for welding inspection of storage tank constructed based on API 620 2012 edition limited to a plate thickness of 10 mm minimum. In case the API 620 does not cover, can I refer to ASME VIII Div.1 2013 (newest edition) which specifies the minimum thickness of 6 mm to be inspected by ultrasonic?

Are there any hierarchy between API Standard 620 and ASME VIII Div.1?

Appreciate you comment.

Regards,
AM. Anang

 
 Reply 
 
anjafo
NDT Inspector
Norway, Joined Aug 2009, 204

anjafo

NDT Inspector
Norway,
Joined Aug 2009
204
19:42 Dec-02-2013
Re: API 620 & ASME VIII Div.1
In Reply to AM Anang at 17:06 Dec-02-2013 (Opening).

Unless you are owner or class society why would you want to do this?
Possibly not to do x-ray?

I feel that you should follow specification that item is being built to and customer request whichever is more stringent.

 
 Reply 
 
collin maloney
NDT Inspector, - Plant Inspector
Applus RTD, Australia, Joined Nov 2000, 147

collin maloney

NDT Inspector, - Plant Inspector
Applus RTD,
Australia,
Joined Nov 2000
147
05:58 Dec-04-2013
Re: API 620 & ASME VIII Div.1
In Reply to AM Anang at 17:06 Dec-02-2013 (Opening).

Hi
Very simple, API is the superintendant code, so if they say 10mm is the limit then thats what it is.
API 650 and 620 both refer to ASME VIII, but if you read the API code carefully, they use ASME when they dont want to reinvent the wheel!

 
 Reply 
 

Product Spotlight

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Navic - Steerable Modular Automated Scanner

The Navic is a modular, motorized, steerable scanner designed to carry multiple attachments used
...
in various scanning and inspection applications. The Navic is capable of weld scanning (girth welds and long seam welds), automated corrosion mapping, and tank scanning.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window