EXTREME VALUE STATISTIC

Dear all:

Can anybody tell me what is the "Extreme Value Statistic" means? Also, could anybody tell me where I can get sone information about the "Extreme Value Statictics"?


 
 Reply 
 
Kris Van de Rostyne
Kris Van de Rostyne
06:49 Mar-24-2003
Re: EXTREME VALUE STATISTIC
: Dear all:
.
: Can anybody tell me what is the "Extreme Value Statistic" means? Also, could anybody tell me where I can get sone information about the "Extreme Value Statictics"?
.
Hello,
Extreme value statistics is used in NDT to describe the statistical behavior of local corrosion phenomena like e.g. pitting corrosion. E.g. Leaking of a container will result as soon as ONE ('extreme') pit is as large as the container wall thickness. To predict a maximum expected pit depth from a limited set of measurements, extreme value calculations are required. Care should be taken when sampling the data.
Details can be found in:
*”Introduction to life prediction of industrial plant materials: Application of the extreme value statistical method for corrosion analysis”, editor M. Kowaka, Allerton Press Inc., 1994
*”Extremes: Statistical Theory and Applications in Science, Engineering and Economics”, Editor-in-Chief: H. Rootzén, Kluwer, 1999

Hope this helps,

Kris




 
 Reply 
 
F.Mustapha
F.Mustapha
00:27 Apr-21-2005
Re: EXTREME VALUE STATISTIC
: : Dear all:
: .
: : Can anybody tell me what is the "Extreme Value Statistic" means? Also, could anybody tell me where I can get sone information about the "Extreme Value Statictics"?
: .
: Hello,
: Extreme value statistics is used in NDT to describe the statistical behavior of local corrosion phenomena like e.g. pitting corrosion. E.g. Leaking of a container will result as soon as ONE ('extreme') pit is as large as the container wall thickness. To predict a maximum expected pit depth from a limited set of measurements, extreme value calculations are required. Care should be taken when sampling the data.
: Details can be found in:
: *”Introduction to life prediction of industrial plant materials: Application of the extreme value statistical method for corrosion analysis”, editor M. Kowaka, Allerton Press Inc., 1994
: *”Extremes: Statistical Theory and Applications in Science, Engineering and Economics”, Editor-in-Chief: H. Rootzén, Kluwer, 1999
.
: Hope this helps,
.
: Kris
.

Principle Component Analysis (PCA) is one of EVS methods that have the capability to reduce dimension in vectorial form of data. Try any search engine to get this definition or if you're in doubt you can contact me and i'll send few journals paper that relates with this statistical approaches.

cheers



 
 Reply 
 

Product Spotlight

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

FD800 Bench Top Flaw Detectors

The bench-top FD800 flaw detector range combines state-of-the-art flaw detection with advanced mater
...
ial thickness capabilities. Designed for use in the laboratory these gauges are the tool you need for all your flaw detecting needs.
>

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window