deepak
India, Joined Mar 2012, 2

deepak

India,
Joined Mar 2012
2
08:22 Jun-10-2014
Fillet weld tests

Sir,

How i can inspect the fillet welds (NDT).
Which NDT method is used for testing for production fillet weld.
Is UT is applicable for Fillet weld?

 
 Reply 
 
Dr Mohamed Blaow
Engineering, researcher
Faculty of engineering, Libya, Joined Mar 2013, 1

Dr Mohamed Blaow

Engineering, researcher
Faculty of engineering,
Libya,
Joined Mar 2013
1
12:15 Jun-10-2014
Re: Fillet weld tests
In Reply to deepak at 08:22 Jun-10-2014 (Opening).

The best technique to use for this particular type of weld is the X-ray or Gamma ray. Aa

 
 Reply 
 
D. Martínez del Valle
Consultant,
Freelance, Spain, Joined May 2013, 188

D. Martínez del Valle

Consultant,
Freelance,
Spain,
Joined May 2013
188
12:32 Jun-10-2014
Re: Fillet weld tests
In Reply to deepak at 08:22 Jun-10-2014 (Opening).

The UT cam be perform if it is specifically indicated, generally the UT is not required by most of international codes and specifications for fillet welds.
The fillet welds, can be examined by PT, or MT, if it can be employed.

 
 Reply 
 

Product Spotlight

GEKKO - Portable Phased Array Testing with TFM in Real-Time

The portable phased array testing system GEKKO provides 64 parallel test channels. On creating testi
...
ng parameters the operator is assisted by the CIVA software. Due to its modular set-up the GEKKO instrument is suitable for operators of all skill levels.
>

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window