Hello,

I am currently looking for a pulsed eddy current system for corrosion detection, but it seems that there are not so much constructors for systems.
I've tried Google, but no luck, only company who do the inspection, but no company who sell the system.

Do someone can help me to find a company who sell systems?

Thanks

Nicolas

 
 Reply 
 
Adel
Adel
14:51 Dec-15-2014
Re: Pulsed eddy current
In Reply to N. CARRION at 09:52 Dec-13-2014 (Opening).

Hello Nicolas,
Can you please more describe the corrosion that you try to detect and the application.
Probably I have a solution for you.

Regards,

Adel

 
 Reply 
 
N. CARRION
N. CARRION
09:23 Dec-17-2014
Re: Pulsed eddy current
In Reply to Adel at 14:51 Dec-15-2014 .

Hello Adel, my principal need is thickness measurment under insulation.

Regards

Nicolas

 
 Reply 
 
B. BOUTTIER
R & D,
Veolia Environnement Research & Innovation, France, Joined Apr 2013, 1

B. BOUTTIER

R & D,
Veolia Environnement Research & Innovation,
France,
Joined Apr 2013
1
15:00 Dec-17-2014
Re: Pulsed eddy current
In Reply to N. CARRION at 09:52 Dec-13-2014 (Opening).

Dear Nicolas,

I know you have two manufacturer in the world:
- APPLUS RTD
- ROCKSOLID GROUP

Also, works can be realised by :
- MISTRAS

Best regards,

Bertrand

 
 Reply 
 
N. CARRION
N. CARRION
08:34 Dec-18-2014
Re: Pulsed eddy current
In Reply to B. BOUTTIER at 15:00 Dec-17-2014 .

Bonjour et merci Bertrand, je connaissais déjà le système A+RTD.

The system I have seen seems to come from Shell Global Solutions, I've tried to find something about it, but with no result.
Do someone know if this system is still available, and if yes where I can find it?

Thanks

Nicolas

 
 Reply 
 
D Grindlay
D Grindlay
10:18 Dec-18-2014
Re: Pulsed eddy current
In Reply to N. CARRION at 08:34 Dec-18-2014 .

Nicolas,
To date Applus RTD supply and develop the Incotest system, and Shell Global solutions both use and license the PEC to service companies. I believe Oceaneering use the PEC system.

http://www.applusrtd.us/en/service/RTD_INCOTEST-1340227850323

http://www.oceaneering.com/oceandocuments/brochures/inspection/INS%20-%20Pulsed%20Eddy%20Current%20(PEC).pdf

Hope this helps
Regards
Darren

 
 Reply 
 
Frank Lund
R & D,
United Kingdom, Joined Apr 2005, 222

Frank Lund

R & D,
United Kingdom,
Joined Apr 2005
222
13:51 Dec-18-2014
Re: Pulsed eddy current
In Reply to N. CARRION at 08:34 Dec-18-2014 .

Nicolas,

I recall talking with Shell about that (Quentin Sjipkens is a name that springs to mind but I may well have it wrong).

NDT.NET has an article on it

http://www.ndt.net/forum/files/pec-offshore.pdf

And TUV refers to it.

http://www.tuv.com/en/corporate/business_customers/materials_testing_and_inspection/advanced_ndt/pulsed_eddy_current/pulsed_eddy_current.html

Cheers,

Frank

 
 Reply 
 

Product Spotlight

MUSE Mobile Ultrasonic Equipment

The MUSE, a portable ultrasonic imaging system, was developed for in-field inspections of light-weig
...
ht structures. The MUSE consists of a motor-driven manipulator, a water circulation system for the acoustic coupling and a portable ultrasonic flaw detector (USPC 3010). The MUSE provides images of internal defects (A-, B-,C- and D-scan).
>

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

NOVO Armor 15 & NOVO Armor 22

The Armor Kit Contains the NOVO Armor, which provides additional mechanical protection to the NOVO 1
...
5WN & NOVO 22WN Detectors, the Armor Stand and a traveling soft cover. - Newest shock absorbent technology case - Water resistant design - Supports wired & wireless communication - Multiple positioning options - Tripod connection using the Built-in 1/4” threads - Simple Detector battery replacement
>

Echomac® PA Bar Tester

The Echomac® PA BT provides 100% inspection of round bars for core and surface defects, at speeds u
...
p to 2 m/sec, depending on the specific application. The unit allows producers to handle a much larger range of diameters in one installation, and is available in 3 models to test 10 – 75mm diameter (small model); 20 – 130mm (medium model) or 50 – 254mm (large model) bars.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window