Dear Sir,
i need guidance regarding AWS D1.1 code.
sir, we can do PAUT lieu of RT by using AWS D1.1 code.







THANKS......

 
 Reply 
 
J Mark Davis
Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama, USA, Joined Mar 2000, 85

J Mark Davis

Teacher, And Consultant
University of Ultrasonics, Birmingham, Alabama,
USA,
Joined Mar 2000
85
20:52 Apr-03-2015
Re: PAUT
In Reply to sandip at 13:59 Apr-03-2015 (Opening).

Yes you can iaw paragraph 6.36 and 6.36 if you qualify your PA procedure and your personnel.

AWS D1.5 has adopted the new Annex K for Phased Array that I developed for the 2015 AWS if approved by AASHTO. Which should happen this year. I have presented to TAC which as far as I understand has approved the new Annex K.

I have developed a draft ballot for D1.1 to be review by D1Q. I will make the final presentation next week in Miami. But they say it will not make it until 2020 code.

BUT, under todays rules if the engineer of record approves Phased Array then you can if you follow 6.36 and 6.37.

Several companies have used PA successfully with engineering approval

We have qualified PA procedures and personnel for these entities.

Sincerely,

J. Mark Davis
Davis NDE, Inc.

 
 Reply 
 
SANDIP
NDT Inspector,
India, Joined Dec 2014, 7

SANDIP

NDT Inspector,
India,
Joined Dec 2014
7
14:26 Apr-04-2015
Re: PAUT
In Reply to J Mark Davis at 20:52 Apr-03-2015 .

Thanks for your valuable opening.
sir. I wont to make a calibration block. for paut pipe to pipe butt joint 4" pipe thickness is 13.5mm according to the DNV- OS-F101, sir i just wont know about reference reflector. what i have to make there. SDH/NOTCH.

 
 Reply 
 
Ed Ginzel
R & D, -
Materials Research Institute, Canada, Joined Nov 1998, 1307

Ed Ginzel

R & D, -
Materials Research Institute,
Canada,
Joined Nov 1998
1307
15:48 Apr-04-2015
Re: PAUT
In Reply to SANDIP at 14:26 Apr-04-2015 .

Sandip, you will need to specify which appendix in OS-F101 you are working to. Appendix D is for all NDT except automated UT of girth welds. Appendix E is for automated UT of girth welds. Appendix D is essentially the typical UT requirements and the description for procedures are found in DNV Classification note 7. Table D-1 in F101 provides the details of the requirements for the sensitivity calibration blocks. If automated UT (AUT) is planned for your project, DNV OS F101 "demands" a system qualification. You may use virtually any reference target sizes or shapes, but you must demonstrate reliability (with a 90|95 PoD) and you must quantify your sizing accuracy. The qualification process is described in Section H of Appendix E and invokes the requirements of DNV RP-118. You may find this process particularly demanding for sizing if using an ECA based acceptance criteria. Section H in Appendix E requires under sizing error tolerances giving less than or equal to 5% probability of under sizing be determined and used in relation to any ECA specified defect sizes.

 
 Reply 
 

Product Spotlight

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

HARDNESS TESTER TKM-459CE combi

TKM-459CE combi applies 2 methods of hardness control: UCI and Leeb. It provides high-accuracy tes
...
ting of metals and alloys as well as items of different sizes and configurations, their hardened layers and galvanic coatings. Device represents results in HB, HRC, HV and others. Shock-, dust- and water-proof housing with intuitive software make this gauge easy to use in all working conditions.
>

OPBOX with standard software is able to do all types of inspections and measurements: flaw detection in welds and materials, scanning of objects, testing composite materials, forged and moulded pieces, many UT inspections, measurements of properties of ma

Typical applications: UT measurements with pulse technique, Measurement of thicknesses also at hig
...
h temperatures, Measurements of properties of materials, including fluids and gases We are delivering a standard version of the software (for any Microsoft Windows up to 10 x64 with Microsoft Hardware certification report Approved) and for special needs: SDK with ready to use examples for LabView, MATLAB x64, C++ wrapper for dll, Python and Linux., and also low-level description of how to control our devices directly from any USB tools
>

Magnetic X-Ray Pipeline Crawler 6''-60''

Suitable to work in 6''-60''diameter with speed of up to 18m/min, Max. moving diatance 5 kilometer
...
s and provide the efficient inspection of the pipeline.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window