08:40 Oct-10-2003
Ultrasonics for Cement Lining

1) Is there any Ultrasonic technique to measure lining/ coating thickness on steel pipes?

2) Can dual probes help in this regard?

Your valuable replies shall be appreciated.

Regards



 
 Reply 
 
Todd Allen
Consultant, Ground Penetrating Radar ( GPR )
Radarview Concrete and Underground 3D Imaging, USA, Joined Jan 2003, 7

Todd Allen

Consultant, Ground Penetrating Radar ( GPR )
Radarview Concrete and Underground 3D Imaging,
USA,
Joined Jan 2003
7
01:41 Oct-13-2003
Re: Ultrasonics for Cement Lining
----------- Start Original Message -----------
: 1) Is there any Ultrasonic technique to measure lining/ coating thickness on steel pipes?
: 2) Can dual probes help in this regard?
: Your valuable replies shall be appreciated.
: Regards
------------ End Original Message ------------

Hello,

Yes, there are a few methods that could be used to measure the thickness of concrete / cement linings and or coatings. The 1st is Ground Penetrating Radar which will measure the thickness of the concrete by detecting the strong dielectric change at the concrete-steel interface. This method must be done from the concrete side not the steel side.
The 2nd method is Impact Echo testing which essentially uses very low frequency impacts on the concrete surface. The frequency response from the echo at the interface can be correlated to a thickness.
The 3rd method would be to use Radiography to get a profile image of the pipe. This method may/may not work depending on the size and thickness of the pipe and concrete.

Thanks,
Todd Allen
Radarview Structural and Underground Services
281-705-9476


 
 Reply 
 
Bijay Muduli
Engineering
IOCL, India, Joined Jul 2003, 4

Bijay Muduli

Engineering
IOCL,
India,
Joined Jul 2003
4
02:08 Oct-16-2003
Re: Ultrasonics for Cement Lining
----------- Start Original Message -----------
: : 1) Is there any Ultrasonic technique to measure lining/ coating thickness on steel pipes?
: : 2) Can dual probes help in this regard?
: : Your valuable replies shall be appreciated.
: : Regards
: Hello,
: Yes, there are a few methods that could be used to measure the thickness of concrete / cement linings and or coatings. The 1st is Ground Penetrating Radar which will measure the thickness of the concrete by detecting the strong dielectric change at the concrete-steel interface. This method must be done from the concrete side not the steel side.
: The 2nd method is Impact Echo testing which essentially uses very low frequency impacts on the concrete surface. The frequency response from the echo at the interface can be correlated to a thickness.
: The 3rd method would be to use Radiography to get a profile image of the pipe. This method may/may not work depending on the size and thickness of the pipe and concrete.
: Thanks,
: Todd Allen
: Radarview Structural and Underground Services
: 281-705-9476
------------ End Original Message ------------

Thank you verymuch Mr Allen.




 
 Reply 
 

Product Spotlight

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

TESTD-PT SYSTEM

Pulse thermography is a non-contact test method that is ideal for the characterization of thin fil
...
ms and coatings or the detection of defects. With a remarquable short test time and a high detection sensitivity, the Telops TESTD-PT is the perfect tool for non- destructive testing. With such high frame rates, it is even possible to investigate highly conductive or diffusive materials.
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>