Help! - c-scan test panel

I am currently doing a BEng in mechanical engineering and in my second year have decided to reasearch C-Scan and create a test panel. This reasearch will be continued into my third year therefore it is necessary that I do everything correctly now.

I have no experience at all of NDT or Ultrasonics.

Can any body enlighten me in simple terms what can test panels can do exactly and what is the difference to a-scan and c-scan?

Any other information on these topics would be much appreciated.

Regards
Mark


 
 Reply 
 
Neil Burleigh
Sales
Krautkramer Australia Pty Ltd, Australia, Joined Dec 2002, 159

Neil Burleigh

Sales
Krautkramer Australia Pty Ltd,
Australia,
Joined Dec 2002
159
02:50 Nov-16-2003
Re: Help! - c-scan test panel
Hi Mark,
Check out the Krautkramer website go to www.agfandt.com and then click on the Krautkramer Ultrasonics Systems section. The next page you see is all about Ultrasonic testing. At the bottom of the page is a booklet "Introduction to Basic Principles of Ultrasonic Non-destruction Testing". You can download it or they will send you a copy it is about 2.5MB. On the same page you can also get a copy of the Echo 39 magazine on pages 40-43 there are two articles on Cscan presentation and associated equipment. From pages 33-39 there are articles on various Ultrasonic flaw detectors with Ascan presentation.
Hope this sets you off in the right direction for your research.
Regards
Neil Burleigh


----------- Start Original Message -----------
: I am currently doing a BEng in mechanical engineering and in my second year have decided to reasearch C-Scan and create a test panel. This reasearch will be continued into my third year therefore it is necessary that I do everything correctly now.
: I have no experience at all of NDT or Ultrasonics.
: Can any body enlighten me in simple terms what can test panels can do exactly and what is the difference to a-scan and c-scan?
: Any other information on these topics would be much appreciated.
: Regards
: Mark
------------ End Original Message ------------




 
 Reply 
 
Rolf Diederichs
Director,
NDT.net, Germany, Joined Nov 1998, 617

Rolf Diederichs

Director,
NDT.net,
Germany,
Joined Nov 1998
617
07:09 Nov-17-2003
Re: Help! - c-scan test panel
In this month's issue you can find a video presentation of C-scan:
www.ndt.net/article/v08n11/passi2/passi2.htm

In the UT Encyclopedia you find description of:
A-scan: www.ndt.net/article/az/ut/asc.htm
C-scan: www.ndt.net/article/az/ut/csc.htm


----------- Start Original Message -----------
: I am currently doing a BEng in mechanical engineering and in my second year have decided to reasearch C-Scan and create a test panel. This reasearch will be continued into my third year therefore it is necessary that I do everything correctly now.
: I have no experience at all of NDT or Ultrasonics.
: Can any body enlighten me in simple terms what can test panels can do exactly and what is the difference to a-scan and c-scan?
: Any other information on these topics would be much appreciated.
: Regards
: Mark
------------ End Original Message ------------




 
 Reply 
 
David LAVASTRE
Engineering,
EDF CEIDRE, France, Joined Nov 2003, 11

David LAVASTRE

Engineering,
EDF CEIDRE,
France,
Joined Nov 2003
11
04:50 Nov-18-2003
Re: Help! - c-scan test panel
Mark,
You can find interesting informations about Ultrasonic testing (and other testing methods...) at

http://www.ndt-ed.org/


also you can find informations about C-Scan systems at :

http://www.aims.nl/
http://www.scanmaster-irt.com/
http://www.gepower.com/businesses/ge_panametrics/en/index.htm
http://www.karldeutsch.de/
http://www.rd-tech.com/
http://www.agfandt.com/

and a page about the history of C-Scan...(the first C-Scan in the world ;) )
http://www.uxr.com/webpg9.htm

David



 
 Reply 
 

Product Spotlight

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

32:128PR PAUT & 2-ch TOFD Flaw Detector: SyncScan 2

●32:128PR PAUT with optional 2-ch TOFD to maximize your efficiency ●Support PR mode for corrosi
...
on inspection ●Multiple solutions for welds & corrosion ●Faster scan speed (Approximately 3 meters/minute) ●Light weight: 4kg only including battery
>

Research Center IDEKO develops an ultrasonic train wheel inspection system for CAF

The Basque Research centre IK4-IDEKO has developed a state-of-the-art ultrasonic inspection system f
...
or the train wheel. This system secures a sound condition of train wheels and is thus a significant contribution to rail transport safety. The device was delivered to CAF recently and its use allows the manufacturer to become an approved supplier of rolling stock in Italy, as it meets the demanding homologation standards of this country. \\\\r\\\\n
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>