exposure time chart for boiler and structural welds ir 192

Dear friend And Master,
I would like to prepare exposure time chart ir192 for boiler and structural welding... If anyone having this please share it would be grateful. And which penetrameter to use.

Many thanks in advance
Sanjjey

 
 Reply 
 
Michel Couture
NDT Inspector,
consultant, Canada, Joined Sep 2006, 889

Michel Couture

NDT Inspector,
consultant,
Canada,
Joined Sep 2006
889
18:10 Dec-31-2015
Re: exposure time chart for boiler and structural welds ir 192
In Reply to sanjey at 22:54 Dec-29-2015 (Opening).

Sanjey,

No one can give you an exposure chart. Exposure chart have to be done according to all the parameters of the shot like wall thickness, distance source-film distance, strength of the Ir192, film used and so on.

Why don't you do like everyone of us and do the job instead of trying to take short cuts.

 
 Reply 
 
sanjey
sanjey
22:52 Dec-31-2015
Re: exposure time chart for boiler and structural welds ir 192
In Reply to Michel Couture at 18:10 Dec-31-2015 .

Dear Michel,

Thanks for your reply,

I am new to radiography testing could you please share short cut method.

Many thanks
Sanjey

 
 Reply 
 
Michel Couture
Michel Couture
00:58 Jan-01-2016
Re: exposure time chart for boiler and structural welds ir 192
In Reply to sanjey at 22:52 Dec-31-2015 .

Sanjey,

There is no short cut.

 
 Reply 
 
sanjey
sanjey
07:08 Jan-01-2016
Re: exposure time chart for boiler and structural welds ir 192
In Reply to Michel Couture at 00:58 Jan-01-2016 .

Dear Michel,

Thanks Michel... I understood wrongly.

Cheers
Sanjey

 
 Reply 
 
Collin Maloney
NDT Inspector, - Plant Inspector
Applus RTD, Australia, Joined Nov 2000, 147

Collin Maloney

NDT Inspector, - Plant Inspector
Applus RTD,
Australia,
Joined Nov 2000
147
09:49 Jan-03-2016
Re: exposure time chart for boiler and structural welds ir 192
In Reply to sanjey at 07:08 Jan-01-2016 .

Sanjay
Paste the below link into your browser and you can download a "rule of thumb" exposure chart in the section NDT Training Aids - Radiography. Please note that there are commercially available app's to do this as well.

http://www.attar.com.au/download-forms.aspx

 
 Reply 
 
Eric Jacques
Eric Jacques
00:45 Jan-06-2016
Re: exposure time chart for boiler and structural welds ir 192
In Reply to Collin Maloney at 09:49 Jan-03-2016 .

Thank you for the links!
Very good educational materials in there.

EJ

 
 Reply 
 

Product Spotlight

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

PAUT Probes

Typical Phased Array probes have frequencies between 1MHz and 20MHz and the number of wafers is 10
...
to 128. M2 Electronics offers customers conventionally ultrasound probes and the ability to provide high-precision Phased Array Ultrasound Probes of up to 256 wafers. We can also customize the probe for our customers to meet the specific application requirements of the user.
>

HD-CR 35 NDT Computed Radiography System

Portable high-resolution CR scanner for all radiography applications - weld testing, profile images
...
and aerospace. No matter what type of radiographic testing you are performing, the unique TreFoc Technology of the HD-CR 35 NDT imaging plate scanner always guarantees the highest image quality.
>

On-Demand Webinar: Advanced Ultrasonic Techniques for HTHA Detection & Assessment

In the Oil and Gas industry, High Temperature Hydrogen Attack (HTHA) can occur in steels operating a
...
t high temperature, usually above 205°C (400°F). Early stages of HTHA are very difficult to detect. Join us for a webinar presented by Guy Maes, Zetec Sales Engineer Director. The webinar will demonstrate how advanced ultrasonic techniques are deployed for efficient and reliable HTHA inspections.
>