Youn Hyongchan
Youn Hyongchan
08:39 Dec-29-2015
FBH (hole size=0.2mm)

Dear expert

I'd like to make the FBH reference block, but one problem is hole size that are required 0.2mm. Is there anyone to know about the manufacturing company to making 0.2mm FBH?
- Material : STS 304
- Hole size : 0.2mm

Thanks and best regards

 
 Reply 
 
Anmol Birring
Consultant,
Birring NDE Center, Inc., USA, Joined Aug 2011, 786

Anmol Birring

Consultant,
Birring NDE Center, Inc.,
USA,
Joined Aug 2011
786
00:34 Jan-01-2016
Re: FBH (hole size=0.2mm)
In Reply to Youn Hyongchan at 08:39 Dec-29-2015 (Opening).

You can use a larger hole and transfer amplitude based on ratio of areas as per ASTM E-2375, Table 5

 
 Reply 
 
Simon Amallraja
Consultant, Advanced NDT Methods
Anu Consultants, India, Joined Aug 2013, 40

Simon Amallraja

Consultant, Advanced NDT Methods
Anu Consultants,
India,
Joined Aug 2013
40
08:22 Jan-04-2016
Re: FBH (hole size=0.2mm)
In Reply to Youn Hyongchan at 08:39 Dec-29-2015 (Opening).

Contact PH Tools -www.phtools.com and they can help you

 
 Reply 
 
un Hyongchan
Engineering,
KSNT, South Korea, Joined Jan 2016, 2

un Hyongchan

Engineering,
KSNT,
South Korea,
Joined Jan 2016
2
08:28 Jan-04-2016
Re: FBH (hole size=0.2mm)
In Reply to Simon Amallraja at 08:22 Jan-04-2016 .

Many thanks for your reply. I already sent e-mail for this to PH tool. But, they do not answer yet..

 
 Reply 
 
Youn Hyongchan
Engineering,
KSNT, South Korea, Joined Jan 2016, 2

Youn Hyongchan

Engineering,
KSNT,
South Korea,
Joined Jan 2016
2
08:46 Jan-04-2016
Re: FBH (hole size=0.2mm)
In Reply to Anmol Birring at 00:34 Jan-01-2016 .

Thanks for your answer.
When I have ASTM E-2375, I will check it. (that need some time to buy ASTM E-2375).
And, could you please tell me your opinion about below conversion formula that I'm thinking...


- STS 304, #3 FBH (hole size 1.19mm, travel distance 31.75mm(1.25'))
- actual amplitude : 35dB (100% FSH)

0.2mm>
(1) △dB=20 log (P1 / P2)
- P1 or P2 is proportional to area
(2) so, △dB=20 log (area 1 / area 2)^2
=40 log (1.19 / 0.2)
= 30.9 dB
※if #3 FBH are used to standard, 30.9 dB is increased to detect the 0.2mm flaw.



 
 Reply 
 
Phil Herman
Sales, - Manufacture of NDT Reference Standards/Test Blocks
PH Tool Reference Standards, USA, Joined Oct 1999, 79

Phil Herman

Sales, - Manufacture of NDT Reference Standards/Test Blocks
PH Tool Reference Standards,
USA,
Joined Oct 1999
79
17:25 Jan-04-2016
Re: FBH (hole size=0.2mm)
In Reply to Youn Hyongchan at 08:39 Dec-29-2015 (Opening).

Happy New Year Youn Hyongchan.
Thank you for contacting PH Tool on December 20th and also for posting your question on the forum. While the FBH you require for ultrasonic testing is very small (0.2mm diameter) in Type 304 Stainless Steel, it is one that capable test block manufacturers are able to produce. It would be most helpful to know the actual drilled depth of the hole from the entry surface, not the metal travel distance, but how far the drill or EDM electrode must plunge from initial contact.
Phil Herman
President/CEO
PH Tool Reference Standards
www.phtool.com

 
 Reply 
 
Godfrey Hands
Consultant,
PRI Nadcap, United Kingdom, Joined Nov 1998, 304

Godfrey Hands

Consultant,
PRI Nadcap,
United Kingdom,
Joined Nov 1998
304
19:54 Jan-04-2016
Re: FBH (hole size=0.2mm)
In Reply to Youn Hyongchan at 08:46 Jan-04-2016 .

Hi,
Before you spend money on having a test block made, if you add 30.9 dB to your signal with 1.19 mm FBH test block, what will the noise level be like? Will the S/N ratio be one that you could detect this size of defect with?

Godfrey

 
 Reply 
 

Product Spotlight

NEW Wheel Type Phased Array Probe

DOPPLER NEW Wheel Type Phased Array Probe, more stable, new tyre makes lesser acoustic attenuation
...
, much lighter makes easier to handle, more slim size, magnetic and mechanical encoder optional etc...more
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

ISAFE3 Intrinsically Safe Sensor System

ISAFE3 intrinsically safe sensor system of Vallen Systeme is especially targeted at the petrochemica
...
l - as well as oil and gas transportation industry. The sensor system is designed for permanent monitoring or periodic inspection tasks. Sensors are available for different AE-frequency ranges optimized for corrosion and fatigue crack detection and other applications. The ISAFE 3 sensor system consists of an AE-sensor (model ISAS3) certified according to ATEX/IEC for installation in zone 0, gas group IIC, IP68, 20 to +60 °C, and a signal isolator (model SISO3) certified for installation in zone 2. An ISAS3 sensor can be mounted in atmosphere or submerged, e.g. in water or crude oil. It is supported by mounting tools for temporary (magnets) or permanent (welded) installation. ISAFE3 supports automatic sensor coupling test and can be used with any AE signal processor supporting 28V supply at 90 mA peak, e.g. Vallen Systeme ASIP-2/A.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window