Hi,

Can anyone tell me any better film manufacturing brands other than Agfa, Kodak & Fuji ?

Muhammad

 
 Reply 
 
Azhar Iqbal
Other,
TUV Middle East (TUV Nord), United Arab Emirates (UAE), Joined Apr 2006, 36

Azhar Iqbal

Other,
TUV Middle East (TUV Nord),
United Arab Emirates (UAE),
Joined Apr 2006
36
10:16 May-01-2016
Re: NDT Films
In Reply to Muhammad at 09:03 May-01-2016 (Opening).

There is another brand called FOMA from Czech Republic. Their Industrial Films are INDUX R2 to R8 representing C1-C6 and FOMADUX - RX8 (Special Film). These are almost equivalent to Agfa Brand.

 
 Reply 
 
N B Rengaraju
NDT Inspector, NDT Level-III/Radiation Safety Officer(RSO)
Marine and Heavy Engineering Company, MALAYSIA., India, Joined Sep 2014, 106

N B Rengaraju

NDT Inspector, NDT Level-III/Radiation Safety Officer(RSO)
Marine and Heavy Engineering Company, MALAYSIA.,
India,
Joined Sep 2014
106
14:18 May-01-2016
Re: NDT Films
In Reply to Muhammad at 09:03 May-01-2016 (Opening).

Can u tell what's the problem u are currently faving with those brand of films which prompts to look for a more bettet film?

 
 Reply 
 
Csaba Hollo
,
Retired, Canada, Joined Feb 2010, 301

Csaba Hollo

,
Retired,
Canada,
Joined Feb 2010
301
01:27 May-03-2016
Re: NDT Films
In Reply to Muhammad at 09:03 May-01-2016 (Opening).

I am also curious as to what the issue is with Agfa, Carestream(kodak), and Fuji. They make very good radiographic film.

 
 Reply 
 
m
m
13:24 May-11-2016
Re: NDT Films
In Reply to N B Rengaraju at 14:18 May-01-2016 .

Dear N B Rengaraju,

In fact issue is not related to quality ,it more inclined towards the cost of films .

Now a days , NDT market is getting saturated day by day ,competition is increasing .

Intent is to find a good brand which can be price competitive with Agfa & Kodak.

 
 Reply 
 
N B Rengaraju
NDT Inspector, NDT Level-III/Radiation Safety Officer(RSO)
Marine and Heavy Engineering Company, MALAYSIA., India, Joined Sep 2014, 106

N B Rengaraju

NDT Inspector, NDT Level-III/Radiation Safety Officer(RSO)
Marine and Heavy Engineering Company, MALAYSIA.,
India,
Joined Sep 2014
106
15:46 May-11-2016
Re: NDT Films
In Reply to m at 13:24 May-11-2016 .

Dear Muhammad,

In this world, anything of a better quality and performance shall have a premium attached to it. So, you will never be able to get a same quality at same price.
Now, purely from commercial point of view, you can opt for Fuji films, which i feel is more cost competative to Agfa or Kodak. It can perform adequately under ideal conditions of processing. Its durability cannot be equated to Agfa or Kodak brands. This is from my practical experience.
Beyond this, I am not exposed to further cheaper brands and hence cannot comment.
Hope this information is useful to you.

 
 Reply 
 

Product Spotlight

Silverwing RMS PA - Phased-array corrosion mapping

Eddyfi Technologies integrated two market leading solutions, Silverwing’s RMS and M2M’s instru
...
ments to provide a high-speed, remote access ultrasonic phased-array inspection system with live total focusing method (TFM).
>

UCI Hardness Tester NOVOTEST T-U2

UCI hardness tester NOVOTEST T-U2 is is used for non-destructive hardness testing of: metals and
...
alloys by scales of hardness: Rockwell (HRC), Brinell (HB), Vickers (HV); non-ferrous metals, alloys of iron etc., and using five additional scales for calibration; with tensile strength (Rm) scale determines the tensile strength of carbon steel pearlitic products by automatic recalculation from Brinell (HB) hardness scale.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

SITEX CPSERIES

Teledyne ICM’s CPSERIES has been designed with a view to revolutionizing the handling and perfor
...
mances of portable X-Ray sets. Despite having managed to halve the weight of similar portable X-Ray generators available on the market (while continuing to provide the same power output), the SITEX CPSERIES generators feature a shutter, a laser pointer, a beryllium window, an aluminum filter and two integrated diaphragms (customized sizes are available upon request). Without compromising the robustness and reliability for which ICM products are renowned, the small size and light weight of the SITEX CPSERIES will radically change the way that you perform your RT inspections. And you will see a positive impact in terms of both quality and return on investment (ROI).
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window