High sensibilty inspection of Ni-base forgings

Hello everybody !
I have a little question about the immersion UT inspection of powder metallurgy forgings (Ni base alloys).
The required sensibility is FBHØ0.2mm at 80%FSH reject with a detection level at FBHØ0.14mm.
- We use calibration block with FBHØ0.4mm in RENE88 or 95.
Actually the settings give :
- FBHØ0.2mm > 80% (that give a FBHØ0.4mm +12dB sensibility)
- FBHØ0.14mm > -6.19dB of 0.2mm (39.2%)
- using a -2dB beam diameter that gives a gate level at 31.13% (-2dB of 39.2%)to assume required detection level.

Can we work with FBHØ0.4mm at 80% FSH ?
With :
- FBHØ0.2mm > 20%
- FBHØ0.4mm > 9.8%
and a gate level of 7.7% with beam diameter -2dB.

What do you think about this second method ?

David





 
 Reply 
 

Product Spotlight

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

Immersion systems

ScanMaster ultrasonic immersion systems are designed for high throughput, multi shift operation in a
...
n industrial or lab environment. These fully integrated systems provide various scanning configurations and incorporate conventional and phased arrays technologies to support diverse applications, such as inspection of disks, bars, shafts, billets and plates. All of ScanMaster immersion systems are built from high accuracy scanning frames allowing for scanning of complex parts and include a multi-channel ultrasonic instrument with exceptional performance. The systems are approved by all major manufacturers for C-scan inspection of jet engine forged discs. Together with a comprehensive set of software modules these flexible series of systems provide the customer with the best price performance solutions.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

IRIS 9000Plus - Introducing the next generation of heat exchanger inspection.

Representing the seventh generation of the IRIS system, the IRIS 9000 Plus has nearly 200 years of c
...
ombined field inspection experience incorporated in its design. This experience combined with a strong commitment to quality and a history of innovation has made Iris Inspection Services® the undisputed leader in IRIS technology.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window