Consultant,
RNDT, Inc., USA, Joined Jul 2002, 24

Fred Raco, Jr

Consultant,
RNDT, Inc.,
USA,
Joined Jul 2002
24
03:53 Feb-27-2004
UT & RT inspection of butt fusion welds in PVC pipe

We are in the process of starting a research program evaluating butt fused PVC pipe welds. We have located some information already but could use more prior to the start of the project. Is there any information out there that could assist us? Thanks in advance for your help.

Regards,

Fred Raco, Jr.


 
 Reply 
 
Mike Troughton
Mike Troughton
05:15 Mar-01-2004
Re: UT & RT inspection of butt fusion welds in PVC pipe
We have been carrying out research into UT and RT inspection of butt fusion welds in PE pipes for around 15 years and have published many papers on the subject, e.g.

Troughton M J: "Welding with integrated non-destructive examination of polyethylene pipes". Plastics Pipes XI Conference, Munich, Germany, 3-6 September 2001.

Munns I J and Georgiou G A: "Ultrasonic and radiographic NDT of butt fusion welded polyethylene pipes", Insight 41(5), 291.

We are also currently developing new NDT techniques for both butt fusion and electrofusion welds in PE pipes.

PVC pipes are rarely butt fusion welded. They are normally joined using a solvent cement. However, if you are indeed looking to carry out NDT on PVC butt fusion welds, then these papers would be a good starting point.

----------- Start Original Message -----------
: We are in the process of starting a research program evaluating butt fused PVC pipe welds. We have located some information already but could use more prior to the start of the project. Is there any information out there that could assist us? Thanks in advance for your help.
: Regards,
: Fred Raco, Jr.
------------ End Original Message ------------




 
 Reply 
 
ams_ati
ams_ati
08:05 Nov-21-2004
Re: UT RT inspection of butt fusion welds in PVC pipe
i need some information about ndt ( specialy new ndt methods ) in inspection of electrofusion welds in PVC pipe. i'm student of mechanical engineering.
thanks----------- Start Original Message -----------
: We are in the process of starting a research program evaluating butt fused PVC pipe welds. We have located some information already but could use more prior to the start of the project. Is there any information out there that could assist us? Thanks in advance for your help.
: Regards,
: Fred Raco, Jr.
------------ End Original Message ------------





 
 Reply 
 
M. Biglar
M. Biglar
06:35 Feb-06-2005
Re: UT RT inspection of butt fusion welds in PVC pipe
----------- Start Original Message -----------
: We are in the process of starting a research program evaluating butt fused PVC pipe welds. We have located some information already but could use more prior to the start of the project. Is there any information out there that could assist us? Thanks in advance for your help.
: Regards,
: Fred Raco, Jr.
------------ End Original Message ------------

I am a student at mechanical Eng. and start a project about pe pipe joint inspection with N D T method please guide me about this method.
Thanks for your attention



 
 Reply 
 
Udo Schlengermann
Consultant, -
Standards Consulting, Germany, Joined Nov 1998, 180

Udo Schlengermann

Consultant, -
Standards Consulting,
Germany,
Joined Nov 1998
180
06:54 Feb-09-2005
Re: UT RT inspection of butt fusion welds in PVC pipe
as in Feb 2005 the request for UT of welds in PVC pipe appeared again in this forum, a useful information for all readers:

Active from November 2004 there is a new European Standard:
EN 13100-3
Nondestructive testing of welded joints in thermoplastics semi-finished products -
Part 3: Ultrasonic testing

Kind regards
Udo Schlengermann
GE Inspection Technologies GmbH
Huerth, Germany

----------- Start Original Message -----------
: : We are in the process of starting a research program evaluating butt fused PVC pipe welds. We have located some information already but could use more prior to the start of the project. Is there any information out there that could assist us? Thanks in advance for your help.
: : Regards,
: : Fred Raco, Jr.
: I am a student at mechanical Eng. and start a project about pe pipe joint inspection with N D T method please guide me about this method.
: Thanks for your attention
------------ End Original Message ------------





 
 Reply 
 
marjan
marjan
07:55 Sep-17-2005
Re: UT RT inspection of butt fusion welds in PVC pipe
------ Dear sirs
We are a group of employees of National iranian Gas
company(N.IG.C).Polyethylene pipes are used in the gas distribution system
of Iran and we are seeking to provide coupler for electrofusion joints.Our
main problem is joint inspection.Please kindly let us know the answer of the
following questions:

1-what are the inspection methods for electrofusion joints and which
one is preferred?

2-Does NDT "non destructive test"method exist for joint inspection
and if so,what are the equipments and standards and expenses.

3-Does NDT method provide inspection and confirmation the quality
lonely or the DT and NDT should be carried out simultaneously.


Sincerely yours

M.yousefi

----- Start Original Message -----------
: We have been carrying out research into UT and RT inspection of butt fusion welds in PE pipes for around 15 years and have published many papers on thesubject, e.g.
: Troughton M J: "Welding with integrated non-destructive examination of polyethylene pipes". Plastics Pipes XI Conference, Munich, Germany, 3-6 September 2001.
: Munns I J and Georgiou G A: "Ultrasonic and radiographic NDT of butt fusion welded polyethylene pipes", Insight 41(5), 291.
: We are also currently developing new NDT techniques for both butt fusion and electrofusion welds in PE pipes.
: PVC pipes are rarely butt fusion welded. They are normally joined using a solvent cement. However, if you are indeed looking to carry out NDT on PVC butt fusion welds, then these papers would be a good starting point.
: : We are in the process of starting a research program evaluating butt fused PVC pipe welds. We have located some information already but could use more prior to the start of the project. Is there any information out there that could assist us? Thanks in advance for your help.
: : Regards,
: : Fred Raco, Jr.
------------ End Original Message ------------




 
 Reply 
 

Product Spotlight

NEOS III

NEOS III is Logos Imagings lightest DR system. With a built-in battery and internal wireless commu
...
nication, the NEOS III is perfect for users that want to quickly assess an item.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

Varex Imaging Large Field of View (FOV) Digital Detector Arrays (DDAs)

A larger FOV DDA can reduce the space and volume of the X-ray inspection system on the factory floor
...
, enable faster scanning times, better throughput and better resolution images at a lower dose. Customers can also save time and money. With these benefits in mind, Varex Imaging has designed a family of large FOV detectors (4343HE, XRD 1611, 4343DX-I, 4343CT) for our industrial imaging customers.
>

Panther

M2M PANTHER is a phased-array equipment designed for both desktop and industrial applications, offer
...
ing unparalleled performance in a compact unit. It combines the speed required for industrial integrated Phased-Array Ultrasound (PAUT) solutions, with the most complete set of total focusing method (TFM) imaging techniques, making it the ultimate tool for R&D and procedure qualification.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window