11:44 Sep-18-2016
Effects of grain size and arrangements of grain in ultrasonic

Please explain me what are effect of grain size and its arrangements of grain size of steel in ultrasonic testing.how please explain in details.

 
 Reply 
 
BODDU PRADEEP
NDT Inspector,
K-KEM , India, Joined Feb 2016, 32

BODDU PRADEEP

NDT Inspector,
K-KEM ,
India,
Joined Feb 2016
32
16:33 Sep-18-2016
Re: Effects of grain size and arrangements of grain in ultrasonic
In Reply to Mayur at 11:44 Sep-18-2016 (Opening).

Scattering is more if wave length is less than one third of grain size. Me too looking for some useful links to study about this.

 
 Reply 
 
Anmol Birring
Consultant,
Birring NDE Center, Inc., USA, Joined Aug 2011, 785

Anmol Birring

Consultant,
Birring NDE Center, Inc.,
USA,
Joined Aug 2011
785
20:55 Sep-18-2016
Re: Effects of grain size and arrangements of grain in ultrasonic
In Reply to Mayur at 11:44 Sep-18-2016 (Opening).

Larger the grain size, higher is the attenuation

 
 Reply 
 
Morteza
Belgium, Joined Jul 2014, 2

Morteza

Belgium,
Joined Jul 2014
2
09:38 Sep-19-2016
Re: Effects of grain size and arrangements of grain in ultrasonic
In Reply to Mayur at 11:44 Sep-18-2016 (Opening).

The following paper may respond some of your questions. It will show how back-scattered signals are changing in a response to the grain morphology of the weld structure.

''Non-Destructive Ultrasonic Examination of Root Defects in Friction Stir Welded Butt-Joints''

 
 Reply 
 
Morteza
Belgium, Joined Jul 2014, 2

Morteza

Belgium,
Joined Jul 2014
2
19:39 Feb-01-2017
Re: Effects of grain size and arrangements of grain in ultrasonic
In Reply to Morteza at 09:38 Sep-19-2016 .

Download

Download Non-destructive ultrasonic examination of root defects in friction stir welded butt-joints

The paper is attached.
 
 Reply 
 

Product Spotlight

TraiNDE UT

TraiNDE UT is a virtual tool associated with a signal database which simulates real inspection con
...
ditions for numerous applications (Type A/V1 block, DAC block, welds and plates).
>

Combination of Digital Image Correlation and Thermographic Measurements

The combination of measuring results from the digital image correlation (ARAMIS, DIC) and temperat
...
ure measuring data from infrared cameras permits the simultaneous analysis of the thermal and mechanical behavior of test specimens in the materials and components testing field.
>

Eddy Current inspection : RotoETscan Rotating Head

The rotating head RotoETscan detects the presence of longitudinal surface or sub surface defects a
...
t high speed. The rotating head is often installed directly on the production line. It is generally dedicated to the control of long products such as tubes, bars and wires, made of ferrous or non-ferrous material. It can also be used for inspection of small parts (billets).
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window