21:06 Mar-26-2017
17.4 and 15.5 PH - MT

Is it possible to carry out MT on 17.4 PH and 15.5 PH grades?
After solution heat treatment and ageing treatment only?
Thank you.

 
 Reply 
 
angelo
Italy, Joined Nov 2012, 13

angelo

Italy,
Joined Nov 2012
13
21:29 Mar-26-2017
Re: 17.4 and 15.5 PH - MT
In Reply to Ermanno at 21:06 Mar-26-2017 (Opening).

Ermanno,
entrambi gli acciai sono magnetizzabili anche se sono noti per avere permeabilità più bassa.
è preferibile lo stato completamente trattato.
È possibile che si evidenzino indicazioni magnetiche dovute a fasi metallurgiche diverse (eg delta ferrite).
è comunque indispensabile seguire le procedure approvate e utilizzare QQI o simili per verificare l'adeguatezza del campo magnetico

 
 Reply 
 
P V SASTRY
R & D, NDT tecniques metallurgy
TAKEN VRS FROM THE POSITION OF SR. DEPUTY GENERAL MANAGER BHEL CORPORATE R&D, India, Joined Jan 2003, 195

P V SASTRY

R & D, NDT tecniques metallurgy
TAKEN VRS FROM THE POSITION OF SR. DEPUTY GENERAL MANAGER BHEL CORPORATE R&D,
India,
Joined Jan 2003
195
12:09 Mar-28-2017
Re: 17.4 and 15.5 PH - MT
In Reply to Ermanno at 21:06 Mar-26-2017 (Opening).


Yes it is possible to carry out MT on these steels.

Their micro structure consists of basically Martensitic phase, in heat treated condition.

Even after precipitation hardening, their micro structures predominantly consists of Martensite, which is ferromagnetic.

As such both steels can be subjected to MT.

Best wishes

P V SASTRY

 
 Reply 
 

Product Spotlight

FAAST-PA! OEM Patented phased Array for high speed UT inspection

Multiangle, Multifocus, Multifrequency, Multibeam. Instead of stacking UT electronics and having m
...
any PA probes, FAAST-PA is able to transmit all delay laws within ONE single shot in Real time.
>

CIVA 2020 UT Module

CIVA NDE Simulation Software is the world leader of NDT Simulation. The UT simulation Module incl
...
udes: - "Beam computation": Beam propagation simulation - "Inspection Simulation": Beam interaction with flaws or specimens The user can simulate a whole inspection process (pulse echo, tandem or TOFD) with a wide range of probes (conventional, Phased- arrays or EMAT), components, and flaws.
>

Cygnus 6+ PRO Multi-Mode Ultrasonic Thickness Gauge

The Cygnus 6+ PRO thickness gauge is the most advance gauge within the Cygnus range with key featu
...
res including: comprehensive data logging; A-scan and B-scan display; manual gain control; Bluetooth connectivity; and much more. With its unique dual display and three measuring modes (Multiple-Echo, Echo-Echo and Single-Echo), this surface thickness gauge offers maximum versatility for inspections.
>

NDT.net launches mobile-friendly design

NDT.net has revamped its website providing a mobile-friendly design.The front page received a comp
...
letely new design and all other sections are now reacting responsively on mobile devices. This has been a major step to make our website more user- friendly.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window