Technical Discussions
Mikel
Mikel
21:41 Oct-23-2017
DGS-AVG with GE SEB2-0º probe

Has anyone had problems with GE SEB2-0º DGS-AVG evaluation curves? In my case, the 3mm FBH signals from a reference block don't coincide with the corresponding USM35 DGS curve and the ERS sizing error is 1 to 2 mm at diferent depths.
Does anyone know anything about this?
Thanks!

    
 
 
S.Senthilkumar
Engineering, QA/QC/NDT
NOV (National Oilwell Varco), Angola, Joined Mar 2006, 41

S.Senthilkumar

Engineering, QA/QC/NDT
NOV (National Oilwell Varco),
Angola,
Joined Mar 2006
41
10:05 Oct-25-2017
Re: DGS-AVG with GE SEB2-0º probe
In Reply to Mikel at 21:41 Oct-23-2017 (Opening).

If I understand correctly, DGS curve is for particular transducer. Use the GE Reference block it should match. different manufacturer there will be slightly different.

    
 
 
Rick Cahill
Rick Cahill
14:32 Oct-30-2017
Re: DGS-AVG with GE SEB2-0º probe
In Reply to Mikel at 21:41 Oct-23-2017 (Opening).

Confirm that you are using the curve for the SEB2 with zero-degree roof angle and not the curve for a standard SEB2-E, which has a roof angle.

    
 
 
Mikel
Teacher,
GOIERRI SCHOOL, Spain, Joined Dec 2013, 6

Mikel

Teacher,
GOIERRI SCHOOL,
Spain,
Joined Dec 2013
6
19:27 Oct-30-2017
Re: DGS-AVG with GE SEB2-0º probe
In Reply to S.Senthilkumar at 10:05 Oct-25-2017 .

Thanks S.Senthilkumar, but this only occurs with SEB2-0º DGS curve. With other probes DGS curves the results are correct.

    
 
 
THEO MICOTTIS
Italy, Joined May 2013, 76

THEO MICOTTIS

Italy,
Joined May 2013
76
09:17 Oct-31-2017
Re: DGS-AVG with GE SEB2-0º probe
In Reply to Mikel at 19:27 Oct-30-2017 .

Hi Mikel, which are the depths/soundpath to FBH's. Regards Theo

    
 
 
Mikel
Teacher,
GOIERRI SCHOOL, Spain, Joined Dec 2013, 6

Mikel

Teacher,
GOIERRI SCHOOL,
Spain,
Joined Dec 2013
6
09:21 Oct-31-2017
Re: DGS-AVG with GE SEB2-0º probe
In Reply to THEO MICOTTIS at 09:17 Oct-31-2017 .

Hi Theo, the depths/soundpath to FBH's are 50, 80, 120 and 180mm. Have you any idea about the problem?

    
 
 
Ronny
Ronny
09:01 Nov-01-2017
Re: DGS-AVG with GE SEB2-0º probe
In Reply to Mikel at 21:41 Oct-23-2017 (Opening).

Hi Mikel,in my experience,there is no channel for SEB 2-0° in USM 35. So did you make DGS curve in custom channel?

    
 
 
Mikel
Teacher,
GOIERRI SCHOOL, Spain, Joined Dec 2013, 6

Mikel

Teacher,
GOIERRI SCHOOL,
Spain,
Joined Dec 2013
6
17:02 Nov-01-2017
Re: DGS-AVG with GE SEB2-0º probe
In Reply to Ronny at 09:01 Nov-01-2017 .

Sorry!!!! I put USM35 in my first message, but instrument is a USM36

    
 
 
THEO MICOTTIS
Italy, Joined May 2013, 76

THEO MICOTTIS

Italy,
Joined May 2013
76
18:34 Nov-02-2017
Re: DGS-AVG with GE SEB2-0º probe
In Reply to Mikel at 17:02 Nov-01-2017 .

Hi Mikel, I suggest you to make a cross-check of AVG diagram loaded in your equipment with paper AVG diagram of the probe.

    
 
 

Product Spotlight

TOPAZ® 64: Fully Integrated Portable 64 Channel PAUT Instrument with FMC & TFM

Introducing TOPAZ64, the industry’s most intelligent fully integrated, portable 64-channel phased
...
array ultrasound (UT) instrument. TOPAZ64 combines code-compliant phased array UT with the industry’s most advanced full matrix capture (FMC) and total focusing method (TFM) capabilities. Featuring the highest acquisition frequency in its class, high resolution FMC and a 12” multi-touchscreen, users can easily visualize even the smallest flaws. TOPAZ64 can generate a bipolar pulse that provides more acoustic energy versus previous models for punching through thick components. The result is a portable tool that delivers increased inspection coverage, more accurate signals, and the ability to handle all UT inspections in one package. TOPAZ64 is ideal for challenging applications in transportation, oil and gas, manufacturing and power generation.
>

Sci Aps Z-Series Portable Handheld Analysers

The world’s only handheld analyzer that measures carbon content in stainless (yes even L-grades),s
...
teels, and cast irons. Also accepted for low Si analysis for sulfidic corrosion analysis, and is widely used in the power industry for Cr analysis, for flow accelerated corrosion applications.
>

EKOSCAN Phased Array

In order to always fit your needs, EKOSCAN can manufacture any type of UT transducer, either convent
...
ional or Phased Array. As an ISO 9001: 2015 certified company, EKOSCAN is extremely careful as far a material selection and manufacturing processes are concerned. Our probes guarantee our customers the benefits of latest innovations regarding piezo-composite, backing, impedance adaptation layer, etc. Specific probes for hostile environment: high temperature, high pressure, corrosive environment,etc. Specific probes designed to fit your specific application: optimization of every parameter to guarantee you the best detection.
>

Navic - Steerable Modular Automated Scanner

The Navic is a modular, motorized, steerable scanner designed to carry multiple attachments used
...
in various scanning and inspection applications. The Navic is capable of weld scanning (girth welds and long seam welds), automated corrosion mapping, and tank scanning.
>