How to determine if coarse grain in piping

Trying to find out how to determine if a material such as stainless steel is coarse grain or fine grain.

 
 Reply 
 
Diego
Consultant,
Freelance, Spain, Joined May 2013, 188

Diego

Consultant,
Freelance,
Spain,
Joined May 2013
188
17:19 Jan-25-2018
Re: How to determine if coarse grain in piping
In Reply to Freddy Harmon at 16:43 Jan-25-2018 (Opening).

Through metallography

 
 Reply 
 
Andrew Robinson
Sales,
PH Tool Reference Standards, USA, Joined Feb 2012, 4

Andrew Robinson

Sales,
PH Tool Reference Standards,
USA,
Joined Feb 2012
4
19:03 Jan-25-2018
Re: How to determine if coarse grain in piping
In Reply to Freddy Harmon at 16:43 Jan-25-2018 (Opening).

Metallography is the best way, but If you have the Material Test Report from the producing mill, the actual grain size is often listed within. That would be the first place to start, and is completely non-invasive!

I believe it is also possible to determine coarse vs. fine-grain by ultrasonic testing. Determination of the grain size is based on factors such as the attenuation coefficient and acoustic velocity. It certainly wouldn't be as empirical as a metallograph, though; just a way to roughly sort coarse vs. fine.

 
 Reply 
 

Product Spotlight

FMC/TFM

Next generation for Phased Array UT is here now with FMC/TFM! Have higher resolution imaging, impr
...
oved signal to noise ratio, characterize, size and analyze defects better with access to several wave mode views and save raw FMC data for higher quality analysis.  Some of the benefits are:
  • Beautiful Image! Easier to understand what you're looking at
  • Completely focused in entire image or volume
  • Much easier to define setups before inspection
  • Easier to decipher geometry echoes from real defects
  • Oriented defects (e.g. cracks) are imaged better
  • See image from different wave modes from one FMC inspection
  • FMC data can be reprocessed/analyzed without going back to the field
>

NEW - TD Focus-ScanRX

The NEW Next Generation Advanced UT platform, TD Focus ScanRX - Also available as a card stack solut
...
ion. Key Improvements 1. Data acquisition is significantly faster than current design 2. Better aesthetic – closely aligns with HandyScan RX 3. Improved IP rating (Target IP66) 4. Ruggedized housing 5. Connectors are protected from impact and ingress 6. Integrated stand and separate retractable handle easy to keep clean) 7. Touchscreen with ruggedized display glass 8. 3-Axis encoder input
>

Semi-Automated Phased Array Immersion System for Small Composite Parts

Turn-key semi-automated system as an improved and affordable solution for inspection of small comp
...
osite parts. Includes support table, immersion tank, scanner, PA instrument, PC, Analysis software, database, wedge management and other options.
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window