10:03 Feb-16-2018
Surface Eddy Current Testing using Olympus MS5800

is it possible to do surface eddy current testing using Olympus MS5800?

Regards
Nimesh

 
 Reply 
 
Ezequiel
NDT Inspector,
Argentina, Joined Apr 2016, 23

Ezequiel

NDT Inspector,
Argentina,
Joined Apr 2016
23
12:58 Feb-16-2018
Re: Surface Eddy Current Testing using Olympus MS5800
In Reply to Nimesh Acharya at 10:03 Feb-16-2018 (Opening).

Dear Nimesh, yes! It si possible. You need a surface probe.

 
 Reply 
 
P V SASTRY
R & D, NDT tecniques metallurgy
TAKEN VRS FROM THE POSITION OF SR. DEPUTY GENERAL MANAGER BHEL CORPORATE R&D, India, Joined Jan 2003, 195

P V SASTRY

R & D, NDT tecniques metallurgy
TAKEN VRS FROM THE POSITION OF SR. DEPUTY GENERAL MANAGER BHEL CORPORATE R&D,
India,
Joined Jan 2003
195
18:34 Feb-16-2018
Re: Surface Eddy Current Testing using Olympus MS5800
In Reply to Nimesh Acharya at 10:03 Feb-16-2018 (Opening).

Yes you can very well use it. You need to use different probes for surface testing

P V SASTRY

 
 Reply 
 
Anmol Birring
Consultant,
Birring NDE Center, Inc., USA, Joined Aug 2011, 832

Anmol Birring

Consultant,
Birring NDE Center, Inc.,
USA,
Joined Aug 2011
832
04:38 Feb-17-2018
Re: Surface Eddy Current Testing using Olympus MS5800
In Reply to Nimesh Acharya at 10:03 Feb-16-2018 (Opening).

MS 5800 is a overkill for surface inspection .
While it can be used, the machine is designed for multi frequency ECT of tubing.
Surface inspection is done using simpler portable machines.

 
 Reply 
 

Product Spotlight

VOGT Ultrasonics awarded innovation champion

Let go of the old and try something new. VOGT convinced the jury in the 27th round of the TOP 100
...
innovation competition. Our team is very pleased to officially belong to the TOP 100 in Germany!
>

OmniScan™ X3 flaw detector

The OmniScan X3 flaw detector is a complete phased array toolbox. Powerful tools, like total focus
...
ing method (TFM) images and advanced visualization capabilities, enable you to complete your inspection with greater confidence.
>

High-performance Linear Phased Array Probes

Available to order from stock in a range of 5MHz – 7.5MHz and from 16 to 64 elements. Designed w
...
ith piezo-composite elements, Phoenix phased array probes provide high-resolution imaging to maximise sensitivity; accurate ultrasonic detection and sizing of defects in welds; and effective corrosion mapping. Housed in a rugged stainless steel case for on-site industrial NDT applications.
>

NDTkit RT

NDTkit RT, TESTIA's Digital Radiography software The NDTkit product line software for X-ray analysi
...
s. NDTkit RT is a software benefiting from the Ultis kernel which is dedicated to radiographic image analysis. It offers a set of tools and filtering processes to assist RT operators in finding relevant flaws.
>

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window